Preparation and characterization of electrospun PLGA/gelatin nanofibers as a potential drug delivery system

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

3
104
0
2

Year Published

2012
2012
2022
2022

Publication Types

Select...
6
2

Relationship

0
8

Authors

Journals

citations
Cited by 200 publications
(109 citation statements)
references
References 40 publications
3
104
0
2
Order By: Relevance
“…[130] Electrospinning is the most used process to produce PLGA nanofibers, where their physical-chemical properties can be controlled by changing several factors, such as the polymer and/or surfactant concentrations, voltage, viscosity and distance of the tip to the collector. [131] For instance, a composite nanofiber composed by PLGA and hydroxyapatite (HAp) was developed by electrospinning, for recombinant human bone morphogenetic protein-2 (rhBMP-2) delivery. [132] Authors demonstrated that rhBMP-2 was successfully loaded into the composite nanofibers, being released in a controlled manner (2-8 weeks) without loss of its integrity.…”
Section: Poly(lactic-co-glycolic) Acid Nanofibersmentioning
confidence: 99%
“…[130] Electrospinning is the most used process to produce PLGA nanofibers, where their physical-chemical properties can be controlled by changing several factors, such as the polymer and/or surfactant concentrations, voltage, viscosity and distance of the tip to the collector. [131] For instance, a composite nanofiber composed by PLGA and hydroxyapatite (HAp) was developed by electrospinning, for recombinant human bone morphogenetic protein-2 (rhBMP-2) delivery. [132] Authors demonstrated that rhBMP-2 was successfully loaded into the composite nanofibers, being released in a controlled manner (2-8 weeks) without loss of its integrity.…”
Section: Poly(lactic-co-glycolic) Acid Nanofibersmentioning
confidence: 99%
“…Samples were then weighed in the wet condition. 14 The swelling ratio for each sample was calculated according to the following equation:…”
Section: Swelling Indexmentioning
confidence: 99%
“…For lidocaine, drug release rate lasted two weeks. Meng et al [74] worked on Fenbufen (drug) loaded PLGA/gelatin nanofibers, and found that an increase in the content of natural polymer gelatin caused an increase in the release rates of Fenbufen. Nanofibers used as a drug delivery carrier need to accomplish two steps; one is to load the drug cargo, and the other is the controlled release of the drugs.…”
Section: Polymer-based Nanofibers For Drug Deliverymentioning
confidence: 99%
“…It is difficult to get a uniform matrix and requires tedious and elaborate mixing. Meng et al [74] prepared PLGA/gelatin nanofibers integrated with Fenbufen (FBF) drug using a dissolution method. Prior to electrospinning, the composite polymer-drug solution was mixed for 12 h at room temperature.…”
Section: Dissolution/co-electrospinningmentioning
confidence: 99%