2015
DOI: 10.1016/j.electacta.2015.09.042
|View full text |Cite
|
Sign up to set email alerts
|

Facile synthesis of MoO3/carbon nanobelts as high-performance anode material for lithium ion batteries

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
62
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
6
1

Relationship

1
6

Authors

Journals

citations
Cited by 99 publications
(64 citation statements)
references
References 54 publications
2
62
0
Order By: Relevance
“…[66] Typically, 0.1 g of MoO 3 powder together with 0.445 g of S powder (99.5%, Tianjin Guangfu Fine Chemical Research Institute, China) and 0.011 g of CNTs (Nanjing XFNANO Materials TECH Co., Ltd., China) were grinded and sealed in a hardened stainless steel vial under Ar atmosphere in a glove box, followed by a thermal treatment in a conventional tube furnace at 700 °C for 2 h under Ar atmosphere with a ramping rate of 5 °C min −1 . MoO 3 was prepared by a hydrothermal method as described in the previous work.…”
Section: Methodsmentioning
confidence: 99%
“…[66] Typically, 0.1 g of MoO 3 powder together with 0.445 g of S powder (99.5%, Tianjin Guangfu Fine Chemical Research Institute, China) and 0.011 g of CNTs (Nanjing XFNANO Materials TECH Co., Ltd., China) were grinded and sealed in a hardened stainless steel vial under Ar atmosphere in a glove box, followed by a thermal treatment in a conventional tube furnace at 700 °C for 2 h under Ar atmosphere with a ramping rate of 5 °C min −1 . MoO 3 was prepared by a hydrothermal method as described in the previous work.…”
Section: Methodsmentioning
confidence: 99%
“…To characterize the electrochemical performance of NCM-NC hybrids, half-cells with NCM-NC hybrids as anodes were assembled. [10,16] Additionally,t he peak at about 1.88 Vi s attributed to the oxidation of Mo to MoO 3 [Eq. [16] The insertion of Li ions in the hollow NiÀCo skeletons may contribute to the above three signals (Figure S6 ai nt he Supporting Information).…”
Section: Resultsmentioning
confidence: 99%
“…Eur.J.2020, 26,2013 -2024 www.chemeurj.org 2019 Wiley-VCH Verlag GmbH &Co. KGaA, Weinheim frequency region representt he Warburg impedance (Z w )a ssociated with the solid diffusion of Li ions. Moreover, the diffusion coefficient of Li ions (D Li )w as calculated from Equations (13) and ( 14): [10] Z re ¼ R s þR ct þsw À1=2 ð13Þ After cycling, the R f of NCM-NCs reaches am aximum in the 80th cycle and then it gradually decreases.…”
Section: Lithiumreaction Kineticsmentioning
confidence: 99%
See 1 more Smart Citation
“…(2)], which makes a great contribution to the high specific capacity . However, the bulk MoO 3 electrode suffers from slow electrode reaction kinetics and poor cycling performance due to the intrinsically poor electrical conductivity and large volume change of MoO 3 during the Li‐ion insertion/extraction processes . Hence, the application of MoO 3 ‐based anodes in LIBs is hindered.…”
Section: Introductionmentioning
confidence: 99%