Improved Thermal Stability and Wettability Behavior of Thermoplastic Polyurethane / Barium Metaborate Composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

2
13
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 28 publications
(15 citation statements)
references
References 20 publications
2
13
0
Order By: Relevance
“…The most prominent maximum from this series was the first one, at around 29.3 • , followed by smaller ones at 35.9 • , 39.3 • , 43.1 • , and 47.3 • . These data correlated rather well with a TPU diffraction pattern reported in [29]. In contrast with TPU, significant differences were observed for the XRD pattern of TPO in the 2θ angular domain between 40 • and 65 • .…”
Section: Morphological and Structural Properties Of The Composites Basupporting
confidence: 88%
“…The most prominent maximum from this series was the first one, at around 29.3 • , followed by smaller ones at 35.9 • , 39.3 • , 43.1 • , and 47.3 • . These data correlated rather well with a TPU diffraction pattern reported in [29]. In contrast with TPU, significant differences were observed for the XRD pattern of TPO in the 2θ angular domain between 40 • and 65 • .…”
Section: Morphological and Structural Properties Of The Composites Basupporting
confidence: 88%
“…It clearly shows that the prepared nanocomposites have improved thermal stability on incorporation of GHT into the pure polymer matrix. Emre et al studied the thermal stability of the polyurethane/barium metaborate composites and it was observed that the blending of barium metaborate into polymer matrix has improved the thermal behavior of polyurethane which was similar to our findings .…”
Section: Resultssupporting
confidence: 89%
“…Two sharp peaks at 1726 and 1702 cm −1 are correlated to the ester carbonyl group and the carbonyl stretching of the urethane groups. In addition, peaks at 1530 cm −1 and 1230 cm −1 correspond to urethane C-N stretching and N-H bending absorption, respectively [ 49 ]. The characteristic peaks of h -BN can be found in both the h -BN/TPU and ABN/TPU spectra, however, the intensity gets weaker due to the overlapping of the TPU and high-intensity additives peaks [ 27 ].…”
Section: Resultsmentioning
confidence: 99%