Understanding the composition evolution of grain boundaries and grain boundary precipitation at near-atomic scale in aluminum alloys is crucial to tailor mechanical properties and to increase resistance to corrosion and stress corrosion cracking. Here, we elucidate the sequence of precipitation on grain boundaries in comparison to the bulk in a model Al-Zn-Mg-Cu alloy. We investigate the material from the solution heat treated state (475°C), through the very early stages of aging to the peak aged state at 120°C and further into the overaged regime at 180°C. The process starts with solute enrichment on grain boundaries due to equilibrium segregation accompanied by solute depletion in their vicinity, the formation of Guinier-Preston (GP) zones in the solute-enriched grain boundary regions, and GP zones growth and transformation. The equilibrium segregation of solutes to grain boundaries during aging accelerates this sequence compared to the bulk. Analysis of the ~10 nm wide precipitate-free zones (PFZs) adjacent to the solute-enriched grain boundaries shows that the depletion zones are determined by (i) interface equilibrium segregation; (ii) formation and coarsening of the grain boundary precipitates and (iii) the diffusion range of solutes in the matrix. In addition, we quantify the difference in kinetics between grain boundary and bulk precipitation. The precipitation kinetics, as observed in terms of volume fraction, average radius, and number density, is almost identical next to the depletion zone in the bulk and far inside the bulk grain remote from any grain boundary influence. This observation shows that the region influenced by the grain boundaries does not extend beyond the PFZs.
We present sample transfer instrumentation and integrated protocols for the preparation and atom probe characterization of environmentally-sensitive materials. Ultra-high vacuum cryogenic suitcases allow specimen transfer between preparation, processing and several imaging platforms without exposure to atmospheric contamination. For expedient transfers, we installed a fast-docking station equipped with a cryogenic pump upon three systems; two atom probes, a scanning electron microscope / Xe-plasma focused ion beam and a N2-atmosphere glovebox. We also installed a plasma FIB with a solid-state cooling stage to reduce beam damage and contamination, through reducing chemical activity and with the cryogenic components as passive cryogenic traps. We demonstrate the efficacy of the new laboratory protocols by the successful preparation and transfer of two highly contamination- and temperature-sensitive samples—water and ice. Analysing pure magnesium atom probe data, we show that surface oxidation can be effectively suppressed using an entirely cryogenic protocol (during specimen preparation and during transfer). Starting with the cryogenically-cooled plasma FIB, we also prepared and transferred frozen ice samples while avoiding significant melting or sublimation, suggesting that we may be able to measure the nanostructure of other normally-liquid or soft materials. Isolated cryogenic protocols within the N2 glove box demonstrate the absence of ice condensation suggesting that environmental control can commence from fabrication until atom probe analysis.
Analysis and understanding of the role of hydrogen in metals is a significant challenge for the future of materials science, and this is a clear objective of recent work in the atom probe tomography (APT) community. Isotopic marking by deuteration has often been proposed as the preferred route to enable quantification of hydrogen by APT. Zircaloy-4 was charged electrochemically with hydrogen and deuterium under the same conditions to form large hydrides and deuterides. Our results from a Zr hydride and a Zr deuteride highlight challenges associated to accurate quantification of hydrogen and deuterium, in particular associated to the overlap of peaks at low mass-to-charge ratio and of hydrogen/deuterium containing molecular ions. We discuss possible ways to ensure that appropriate information is extracted from APT analysis of hydrogen in a zirconium alloy systems that is important for nuclear power.
Zircaloy-4 (Zr-1.5%Sn-0.2%Fe-0.1%Cr wt. %) was electrochemically charged with deuterium to create deuterides and subsequently analysed with atom probe tomography and scanning transmission electron microscopy to understand zirconium hydride formation and embrittlement. At the interface between the hexagonal close packed (HCP) a-Zr matrix and a face centred cubic (FCC) d deuteride (ZrD 1.5-1.65 ), a HCP z phase deuteride (ZrD 0.25-0.5 ) has been observed. Furthermore, Sn is rejected from the deuterides and segregates to the deuteride/a-Zr reaction front.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.