Theoretical and experimental investigations of the thermoelectric properties of Al-, Bi- and Sn-doped ZnO

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

2
11
0
1

Year Published

2017
2017
2024
2024

Publication Types

Select...
7
2

Relationship

0
9

Authors

Journals

citations
Cited by 50 publications
(15 citation statements)
references
References 39 publications
2
11
0
1
Order By: Relevance
“…A Figura 2 apresenta o difratograma do produto da síntese hidrotermal assistida por microondas do óxido de zinco e seus diferentes tempos (5,10 e 20 minutos) no processo do microondas. Conforme a análise dos resultados confirmou-se o tipo de estrutura wurtzita pela fase hexagonal do óxido de zinco [2,11,[25][26][27][28]. Sendo confirmado, conforme [4], fortes picos de difração aparecendo em 2θ = 31.8°,34.3° e 36.5°, correspondendo aos planos (100), (002) e (101).…”
Section: Resultados E Discussõesunclassified
“…A Figura 2 apresenta o difratograma do produto da síntese hidrotermal assistida por microondas do óxido de zinco e seus diferentes tempos (5,10 e 20 minutos) no processo do microondas. Conforme a análise dos resultados confirmou-se o tipo de estrutura wurtzita pela fase hexagonal do óxido de zinco [2,11,[25][26][27][28]. Sendo confirmado, conforme [4], fortes picos de difração aparecendo em 2θ = 31.8°,34.3° e 36.5°, correspondendo aos planos (100), (002) e (101).…”
Section: Resultados E Discussõesunclassified
“…Speculated from this, solid solution doping reduced the crystallinity of the particles, forming defect energy level in the energy gap. 30 When dispersed in epoxy resin, abundant dangling bonds and unsaturated bonds in X-ZnO SSs facilitated the superior tightness of the modified corrosion coating.…”
Section: Resultsmentioning
confidence: 99%
“…Followed by the eq , the crystallinity of pure ZnO and X-ZnO SSs was calculated to be 99.21%, 96.65%, 98.80%, and 98.12%, respectively. where I a and I c represented the amorphous phase and the cumulative diffraction intensity of the crystalline phase, the constant k here is usually equal to 1. Speculated from this, solid solution doping reduced the crystallinity of the particles, forming defect energy level in the energy gap . When dispersed in epoxy resin, abundant dangling bonds and unsaturated bonds in X-ZnO SSs facilitated the superior tightness of the modified corrosion coating.…”
Section: Resultsmentioning
confidence: 99%
“…The improvement in photocatalytic performance of ZnO has been investigated by adjusting preparation conditions, 27,28 morphology, 7 particle size, 29 dopant agent, 15,16 and crystallinity. 30 Previous studies have shown that the photocatalytic activity of a photocatalyst is seriously dependent on decreasing the particle size and increasing the degree of crystallinity.…”
Section: Introductionmentioning
confidence: 99%