Tensile and Creep Testing of Sanicro 25 Using Miniature Specimens

Abstract: Tensile and creep properties of new austenitic steel Sanicro 25 at room temperature and operating temperature 700 °C were investigated by testing on miniature specimens. The results were correlated with testing on conventional specimens. Very good agreement of results was obtained, namely in yield and ultimate strength, as well as short-term creep properties. Although the creep rupture time was found to be systematically shorter and creep ductility lower in the miniature test, the minimum creep rates were comp… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
16
0

Year Published

2019
2019
2024
2024

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 25 publications
(16 citation statements)
references
References 27 publications
0
16
0
Order By: Relevance
“…Unfortunately, no detailed analysis seems to have been performed for austenitic stainless steels. Published creep curves for Sanicro 25 [25] show the same tertiary behavior as for cold worked copper, indicating that enhanced recovery is the main mechanism. In addition, the strain during primary creep is quite small.…”
Section: Solid Solution Hardeningmentioning
confidence: 70%
See 4 more Smart Citations
“…Unfortunately, no detailed analysis seems to have been performed for austenitic stainless steels. Published creep curves for Sanicro 25 [25] show the same tertiary behavior as for cold worked copper, indicating that enhanced recovery is the main mechanism. In addition, the strain during primary creep is quite small.…”
Section: Solid Solution Hardeningmentioning
confidence: 70%
“…In our model, ε crit represents the strain in the secondary stage. The total experimental rupture strains are about 40-50% at higher stresses [2,25], and these are clear values for ductile rupture. Considering a significant part from tertiary creep, ε crit has been taken as 0.2 in the model.…”
Section: Solid Solution Hardeningmentioning
confidence: 99%
See 3 more Smart Citations