Synthesis and characterization of zirconia- and silica-doped zirconia nanopowders by oxalate processing

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
13
0

Year Published

2010
2010
2020
2020

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 36 publications
(13 citation statements)
references
References 25 publications
0
13
0
Order By: Relevance
“…The increase in pore diameter can be linked to the presence of sulfate ions on the micropore walls, causing tension and rupture, followed by increased micropore volume and diameter 42 . The spectra in the infrared region shown in Figure 5 indicate the presence of a band at 1630 cm -1 that corresponds to scissor bending vibration of the H-O-H bond of the physisorbed molecular water 27,42,46,47 . The samples showed bands centered at 1078 cm -1 with a shoulder at ~ 1220 cm -1 due to the asymmetric Si-O-Si stretching vibrations of transverse-optical (TO 3 ) mode and the longitudinal-optic (LO 3 ) part stretching vibrations, respectively 47 .…”
Section: Characterizationmentioning
confidence: 99%
See 3 more Smart Citations
“…The increase in pore diameter can be linked to the presence of sulfate ions on the micropore walls, causing tension and rupture, followed by increased micropore volume and diameter 42 . The spectra in the infrared region shown in Figure 5 indicate the presence of a band at 1630 cm -1 that corresponds to scissor bending vibration of the H-O-H bond of the physisorbed molecular water 27,42,46,47 . The samples showed bands centered at 1078 cm -1 with a shoulder at ~ 1220 cm -1 due to the asymmetric Si-O-Si stretching vibrations of transverse-optical (TO 3 ) mode and the longitudinal-optic (LO 3 ) part stretching vibrations, respectively 47 .…”
Section: Characterizationmentioning
confidence: 99%
“…Above 700 °C, the loss of mass is associated with the dehydroxilation of the surface 27 . The usually characteristic band of Si-C at 1276 cm -1 for the ZrO 2 -SiO 2 -Me catalyst in the FTIR analysis ( Figure 5) could not be verified due to the small amount of MeSi(OEt) 3 used for synthesis.…”
Section: Characterizationmentioning
confidence: 99%
See 2 more Smart Citations
“…In the case of ZrO 2 addition, based on the literature data indicates the 574 and 732cm −1 bands as being characteristic of the monoclinic phase of zirconia [14], the band at 555 cm −1 could be ascribed to this component in these samples [15]. The band of the monoclinic zirconia phase that occurs at 732 cm 1 overlaps the symmetric Si-O-Si stretching vibrations of the SiO 4 units.…”
Section: Fig 5 Ir Spectra Of the Studied Glazesmentioning
confidence: 88%