Switchable hydrophobic/hydrophilic surface of electrospun poly (l-lactide) membranes obtained by CF4 microwave plasma treatment

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
25
0

Year Published

2015
2015
2022
2022

Publication Types

Select...
9
1

Relationship

1
9

Authors

Journals

citations
Cited by 51 publications
(25 citation statements)
references
References 48 publications
0
25
0
Order By: Relevance
“…Plasma polymerization is known to be a suitable method for the deposition of many biomaterial coatings [8,9]. Plasma polymerization is in the class of plasma-enhanced chemical vapor deposition (PECVD) methods, which are successfully used for example for thin film deposition [10], surface modification [11,12], or growing of nanomaterials [13][14][15]. Plasma deposition of 2-methyl-2-oxazoline and 2-ethyl-2-oxazoline has already been performed in low-pressure radio frequency (RF) discharge [16][17][18].…”
Section: Introductionmentioning
confidence: 99%
“…Plasma polymerization is known to be a suitable method for the deposition of many biomaterial coatings [8,9]. Plasma polymerization is in the class of plasma-enhanced chemical vapor deposition (PECVD) methods, which are successfully used for example for thin film deposition [10], surface modification [11,12], or growing of nanomaterials [13][14][15]. Plasma deposition of 2-methyl-2-oxazoline and 2-ethyl-2-oxazoline has already been performed in low-pressure radio frequency (RF) discharge [16][17][18].…”
Section: Introductionmentioning
confidence: 99%
“…It was found that the electrospinning are one of the attractive methods to alter the wetting behaviour of the polymer surface. 11, 12 A superior hydrophobic piezoelectric solid for wide applications are barely reported.…”
Section: Introductionmentioning
confidence: 99%
“…In brief, a water droplet was dropped onto a flat sample and the contact angle was recorded and then calculated. The instantaneous contact angle obtained within 1 s. At least five contact angle values of various spots were collected to get the final contact angle value [28,29].…”
Section: Structure and Morphologymentioning
confidence: 99%