Structure and photoluminescence of amorphous silicate composites containing ZnO particles synthesized from layered sodium silicate

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
2
0

Year Published

2014
2014
2023
2023

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 11 publications
(4 citation statements)
references
References 48 publications
0
2
0
Order By: Relevance
“…14 The bands from 745 to 467 cm −1 are contributed from symmetric stretching and bending vibrations of Si-O-Si bonds. 31 Furthermore, an absorption at 1462 cm −1 from CO 3 2− groups possibly resulted from the reaction of CO 2 in air with Na 2 SiO 3 during the sample preparation. 29 However, the absorptions for the deactivated Na 2 SiO 3 @Ni/C catalyst became weak (Fig.…”
Section: Biodiesel Productionmentioning
confidence: 99%
“…14 The bands from 745 to 467 cm −1 are contributed from symmetric stretching and bending vibrations of Si-O-Si bonds. 31 Furthermore, an absorption at 1462 cm −1 from CO 3 2− groups possibly resulted from the reaction of CO 2 in air with Na 2 SiO 3 during the sample preparation. 29 However, the absorptions for the deactivated Na 2 SiO 3 @Ni/C catalyst became weak (Fig.…”
Section: Biodiesel Productionmentioning
confidence: 99%
“…Besides that the samples showed the minor phases of Zinc ions, cristobalite and samarium. The intense diffraction peaks revealed the formation of larger crystallites indicating the present of amorphous silica in the sample [13]. The broad diffraction peaks were due to the smaller crystallite sizes of zinc oxides nanoparticles in the samples [14].…”
Section: Resultsmentioning
confidence: 97%
“…Traces of zinc ions merged with cristobalite, willemite or with Zn 2 SiO 4 : Sm located at 2θ=36.23°, 39.00°, and 54.46° indexed as (020),(223), and (063) [9]. To ascertain the features of the zinc oxide nanoparticles incorporated into the silicon dioxide microparticles [12], there is the need to understand the thermal diffusivity of the matrix samples. The (70-X) Zn 2 XSm30SiO 4 samples at X = 0, 1, 3 and 5 wt% revealed exponential gradient decay relationship with the 1000/T axis.…”
Section: Resultsmentioning
confidence: 99%