Lignocellulosic nanofibril aerogel via gas phase coagulation and diisocyanate modification for solvent absorption

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
7
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 29 publications
(8 citation statements)
references
References 32 publications
0
7
0
Order By: Relevance
“…Additionally, since there were more MDI structures, the modified aerogel had greater residual mass after pyrolysis with a higher MDI content. These comparisons clearly demonstrate the benefits of using MDI to maintain CNF’s thermal stability [ 42 ].…”
Section: Resultsmentioning
confidence: 84%
“…Additionally, since there were more MDI structures, the modified aerogel had greater residual mass after pyrolysis with a higher MDI content. These comparisons clearly demonstrate the benefits of using MDI to maintain CNF’s thermal stability [ 42 ].…”
Section: Resultsmentioning
confidence: 84%
“…X-ray photoelectron spectra, including the main elements and carbon-based bonds, were measured to confirm the chemical reactions of TCNF and QCNF Figure d shows low-resolution spectra of the raw material and TCNF and QCNF samples.…”
Section: Resultsmentioning
confidence: 99%
“…The exposure of inner cellulose chains can also be proved by the increased NMR peak at 88 ppm due to the inner cores of the cellulose Carbon-4 region. It was reported that more crystalline regions are located in inner cores of cellulose microfibrils [ 46 ]. Thus, HTP could cause the increasing CrI as calculated from NMR spectra based on the peaks’ deconvolution and Equation (2) ( Figure S2 ), which correspond to previous studies [ 22 , 47 ].…”
Section: Resultsmentioning
confidence: 99%
“…MB powders were then extracted by toluene/ethanol (2:1, v / v ) for 6 h and oven dried at 60 °C overnight to remove the extractives. To focus on the cellulose and hemicellulose polysaccharides in the samples, lignin was removed by the conventional bleaching method [ 46 , 60 ]. Briefly, the extractive-free samples were treated with sodium chlorite/acetic acid at 75 °C for up to 4 h at the mass/liquid ratio of 1:50.…”
Section: Methodsmentioning