Hydrogen peroxide bleaching of cellulose pulps obtained from brewer’s spent grain

Abstract: Brewer's spent grain (BSG) was evaluated for bleached pulp production. Two cellulose pulps with different chemical compositions were produced by soda pulping: one from the original raw material and the other from material pretreated by dilute acid. Both of them were bleached by a totally chlorine-free sequence performed in three stages, using 5% hydrogen peroxide in the two initial, and a 0.25 N NaOH solution in the last one. Chemical composition, kappa number, viscosity, brightness and yield of bleached and u… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
33
0
4

Year Published

2009
2009
2021
2021

Publication Types

Select...
6
2
1

Relationship

0
9

Authors

Journals

citations
Cited by 62 publications
(38 citation statements)
references
References 24 publications
0
33
0
4
Order By: Relevance
“…Subsequently, the pulp was bleached by a totally chlorine‐free sequence carried out in three stages, using 5% (v/v) hydrogen peroxide in the first two stages and 0.25 mol L −1 NaOH solution in the last stage. Using this procedure, a bleached pulp presenting a kappa number of 11.21, viscosity of 3.12 cP, brightness of 71.3%, cellulose content of 957 g kg −1 and residual lignin of 34 g kg −1 was obtained from BSG …”
Section: Bsg Use In Chemical Processesmentioning
confidence: 99%
“…Subsequently, the pulp was bleached by a totally chlorine‐free sequence carried out in three stages, using 5% (v/v) hydrogen peroxide in the first two stages and 0.25 mol L −1 NaOH solution in the last stage. Using this procedure, a bleached pulp presenting a kappa number of 11.21, viscosity of 3.12 cP, brightness of 71.3%, cellulose content of 957 g kg −1 and residual lignin of 34 g kg −1 was obtained from BSG …”
Section: Bsg Use In Chemical Processesmentioning
confidence: 99%
“…Hal ini dikarenakan lignin pada proses manufaktur kertas akan menurunkan tingkat kecerahan (brightness) sehingga harus dihilangkan secara maksimal, sedangkan hemiselulosa pada kandungan tinggi dapat menurunkan sifat mekanik paper karena adanya penurunan resistensi individu seratnya. Selain itu, adanya hemiselulosa juga menurunkan sifat optik (transparansi) karena sifatnya yang keruh (opacity) (Mussatto, Rocha, dan Roberto 2008). NaOCl 2 , berbentuk kristal putih adalah bahan pemutih serat selulosa yang lembut yang tidak akan merusak secara dekstruktif bahkan jika diproses pada temperatur yang tinggi 100 ᵒC selama beberapa jam (Rahmidar, Nurilah, dan Sudiarty 2018;Putera 2012) 37,6 ± 0,3 23,9 ± 0,3 38,5± 0,0 TKS delignifinasi NaOH 73,0 ± 0,2 14,9 ± 0,2 12,1 ± 0,5 TKS hasil pemutihan NaClO2 1x pemutihan 81.5 ± 2,1 12,7 ± 0,0 5,8 ± 2,1 NaClO2 2x pemutihan 84,1 ± 0,0 12,7 ± 0,1 3,2 ± 0,1 NaClO2 3x pemutihan 84,3 ± 0,3 12,6 ± 0,1 3,1 ± 0,2 Selulosa Standar 80,8 16,6 2,6…”
Section: Pemutihan Dengan Naclounclassified
“…Diferentes tecnologias têm sido desenvolvidas no campo da aplicação do peróxido de hidrogênio. Atualmente a combinação do peróxido de hidrogênio e dióxido de cloro se tornou a maneira mais eficiente de branquear polpas sem cloro elementar (ECF), e peróxido de hidrogênio com oxigênio e ozônio a mais eficiente em polpas totalmente livres de cloro (TCF) [71], [72], [73], [74].…”
Section: Métodos De Obtenção De "Microfibras" E "Nanofibras" De Celulunclassified