Features of the surface morphology of brass and bronze upon irradiation with a high power ion beam

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
5
0

Year Published

2014
2014
2022
2022

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 11 publications
(6 citation statements)
references
References 3 publications
1
5
0
Order By: Relevance
“…Craters induced by inclusion have often been mentioned in past studies [21][22][23][24]. The experimental data of this study are in agreement with previously published results [23,24].…”
Section: Elemental Composition Of the Cratersupporting
confidence: 93%
See 1 more Smart Citation
“…Craters induced by inclusion have often been mentioned in past studies [21][22][23][24]. The experimental data of this study are in agreement with previously published results [23,24].…”
Section: Elemental Composition Of the Cratersupporting
confidence: 93%
“…According to previous studies, possible mechanisms for the creation of a crater are (a) bombardment of the melted surface by the accelerator elements (a technological factor) [12,13]; (b) formation of pores in the surface layer of the sample due to casting [13]; and (c) instability in the physical and chemical states of the irradiated surface [7,12,[21][22][23][24], including differences in phase and chemical composition, impurity distribution, and dislocation density of targets. Few other studies have also suggested filamentation of the ion beam in the pulse [10] and formation of a gas-plasma phase during the ablation of surface volatiles [12] as possible mechanisms for the creation of craters.…”
Section: Elemental Composition Of the Cratermentioning
confidence: 99%
“…As an increase in the ion dose, this led to increase the amorphous lattice site in terms of crater formation. 21 Crater can be observed at the central part of the Figure 2C, and nickel concentration was present in the form of patches at the ridges of that crater. Small particles were present inside the crater can be seen in subsize figure (c).…”
Section: Resultsmentioning
confidence: 97%
“…11f), the craters formed. There are many rea-sons for the generation of craters (such as the preferential vaporization of low melting point elements [59,60] or the hitting of impurities from ion source diode on the material surface [61], etc. ), but there is no unified statement so far.…”
Section: The Effects Of Hipib Irradiation On Microstructure Surface Morphology and Mechanical Property Of Cocrfemnni Heamentioning