Cytocompatibility of HEMA–free resin–based luting cements according to application protocols on dentine surfaces

Abstract: HEMA-free Rely X ARC cement caused greater toxicity to odontoblast-like MDPC-23 cells than did Rely X Unicem cement when both resin-based luting materials were applied to dentine as recommended by the manufacturer.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
20
0

Year Published

2017
2017
2023
2023

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 17 publications
(21 citation statements)
references
References 47 publications
(69 reference statements)
1
20
0
Order By: Relevance
“…Dentin discs (0.4 mm thick; n=56) were obtained from healthy human third molars (Process #32272114.9.0000.5188; Ethics Committee in Research of the Health Sciences Center of the Federal University of Paraíba, Brazil), as described in detail by Soares et al (11). The discs were ground wet with 400-and 600-grit abrasive papers (Carborundum Abrasives, Recife, PE, Brazil) to a set thickness at 0.4 mm, measured by digital caliper (Model 500-144B; Mitutoyo South America Ltda., Suzano, SP, Brazil).…”
Section: Preparation Of Dentin Discsmentioning
confidence: 99%
See 4 more Smart Citations
“…Dentin discs (0.4 mm thick; n=56) were obtained from healthy human third molars (Process #32272114.9.0000.5188; Ethics Committee in Research of the Health Sciences Center of the Federal University of Paraíba, Brazil), as described in detail by Soares et al (11). The discs were ground wet with 400-and 600-grit abrasive papers (Carborundum Abrasives, Recife, PE, Brazil) to a set thickness at 0.4 mm, measured by digital caliper (Model 500-144B; Mitutoyo South America Ltda., Suzano, SP, Brazil).…”
Section: Preparation Of Dentin Discsmentioning
confidence: 99%
“…The discs were ground wet with 400-and 600-grit abrasive papers (Carborundum Abrasives, Recife, PE, Brazil) to a set thickness at 0.4 mm, measured by digital caliper (Model 500-144B; Mitutoyo South America Ltda., Suzano, SP, Brazil). Then, a 0.5 mol/L EDTA solution was applied to each surface for 60 s to remove the smear layer, followed by washing in deionized water for the same period (11). The discs were adapted to a filtration chamber, and a cannula was connected to a 1.80-m column of water through a 0.5-mm-diameter polyethylene tube.…”
Section: Preparation Of Dentin Discsmentioning
confidence: 99%
See 3 more Smart Citations