Characterization of structure and properties of TiN–TiB2 nano-composite prepared by ball milling and high pressure heat treatment

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
10
1

Year Published

2009
2009
2018
2018

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 22 publications
(12 citation statements)
references
References 17 publications
0
10
1
Order By: Relevance
“…Fine grain titanium nitride powders can be synthesized by ball milling of titanium with boron nitride, nitrogenous organic solution, nitrogen gas or ammonia gas at room temperature [9][10][11][12]. Such obtained titanium nitride powders usually have some impurities, which are hard to remove.…”
Section: Introductionmentioning
confidence: 99%
“…Fine grain titanium nitride powders can be synthesized by ball milling of titanium with boron nitride, nitrogenous organic solution, nitrogen gas or ammonia gas at room temperature [9][10][11][12]. Such obtained titanium nitride powders usually have some impurities, which are hard to remove.…”
Section: Introductionmentioning
confidence: 99%
“…The fabrication and properties of the TiN-TiB 2 composites are also reported in many literatures [26][27][28][29][30]. Shobu et al produced TiN-TiB 2 composites by conventional sintering [26] and hot pressing [27] of TiN and TiB 2 powders.…”
Section: Resultsmentioning
confidence: 92%
“…The reactive hot pressing of Ti and BN mixtures at 1600 • C [29] resulted in not complete densification process (only 88.8% RD) and thus decreasing of hardness to 16.8 (±2.33) GPa (Table 3). Qiu et al [30] reported about completely conversion of the ball milled Ti + BN powder mixtures to form TiN-TiB 2 using high pressure heat treatment (HPHT) at 1300 • C and 5 GPa. However, the hardness was only 8.84 GPa and no any presented data about density and K IC of that CCs.…”
Section: Resultsmentioning
confidence: 99%
“…L.X. Qiu et al [93] synthesized of TiN-TiB 2 nano-composite by mechanical milling of mixture of Ti and hexagonal boron nitride (h-BN) and subsequent sintering under high pressure and high temperature. A TiN-TiB 2 composite was fabricated by ball milling of the mixture for 70 h and then sintering at 5 GPa, 1300℃.…”