A Comparative Study of Polymer Insulating Materials Undern Salt-Fog Conditions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
11
0

Year Published

1991
1991
2019
2019

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 55 publications
(11 citation statements)
references
References 5 publications
0
11
0
Order By: Relevance
“…This shows that at higher temperature the Langmuir model breaks down, as it predicts a steady increase. A possible explanation for the qualitative differences at higher temperatures, is that the NaCl solution irreversible changes the substrate composition, through matrix degradation and/or fillers dissolution as explained in 2.2 [9,10,23]. The mechanism of this degradation will be further analyzed in the Sections 4.5, 4.6 and 4.7.…”
Section: Permeation Of Water Into Silicone Rubbermentioning
confidence: 99%
“…This shows that at higher temperature the Langmuir model breaks down, as it predicts a steady increase. A possible explanation for the qualitative differences at higher temperatures, is that the NaCl solution irreversible changes the substrate composition, through matrix degradation and/or fillers dissolution as explained in 2.2 [9,10,23]. The mechanism of this degradation will be further analyzed in the Sections 4.5, 4.6 and 4.7.…”
Section: Permeation Of Water Into Silicone Rubbermentioning
confidence: 99%
“…A few diagnostic techniques which have been commonly used are discussed in Aging of polymeric arrester (or insulator) housing materials is not closely related to the magnitude of leakage currents on the housings. This has been demonstrated by many researchers [3]. As an example, one can often measure much higher leakage currents or watts loss on porcelain housed arresters than on polymer housed arresters, yet one would not claim that porcelain housings age more rapidly than polymer.…”
Section: Discussionmentioning
confidence: 99%
“…Now that acceptable surge arrester performance under these conditions has been demonstrated, today's emphasis on testing is on evaluating polymer housing performance under various climatic conditions [2,3,4,51.…”
Section: Introductionmentioning
confidence: 99%
“…Water of hydration could hinder the physical accumulation of residue on the surface, because of the physical cleaning action of the water on the surface [33], [34]. In particular, the water of hydration released during the dehydration of ATH may scatter the residue.…”
Section: The Role Of Inorganic Fillers In Sir DC Insulationmentioning
confidence: 99%