Rechargeable Zn‐MnO2 batteries are boosted by the reversible intercalation reactions in mild aqueous electrolytes, but they still suffer from cathode degradation. Herein, Zn‐MnO2 batteries with high durability and high energy density are achieved by supplementing MnO2 deposition and dissolution in a mild aqueous electrolyte. The main finding is that adjusting Mn2+ concentration to a critical range enables a reversible MnO2/Mn2+ redox conversion without the involvement of oxygen evolution. This can recycle the by‐products from MnOOH disproportionation (MnOOH → MnO2 + Mn2+), resulting in a battery with extremely high durability (16 000 cycles without obvious capacity fading), high energy density (602 Wh kg−1 based on the active mass of the cathode), and high‐rate capacity (430 mAh g−1 at 19.5 A g−1). The utilization of a 3D carbon nanotube foam skeleton can accommodate the volume change during MnO2 deposition/dissolution and provide paths for efficient charge and mass transport. This work provides a feasible way to push the development of Zn‐MnO2 batteries in mild aqueous electrolytes.
Confining Zn plating and stripping in a robust and conductive 3D carbon nanotube network results in an electrode, which shows excellent reversibility at high depth of discharge and enables zinc-ion batteries with high-rate and long-term performance.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.