The current laboratory study is evaluating the effect of hydrofluoric acid etching duration on the surface characteristics of five silica-based glass ceramics. Changes in the pore pattern, crystal structure, roughness, and wettability were compared and evaluated. Seventy-five rectangularly shaped specimens were cut from each material (IPS e-max™, Dentsply Celtra™, Vita Suprinity™, Vita mark II™, and Vita Suprinity FC™); the sectioned samples were finished, polished, and ultrasonically cleaned. Specimens were randomly assigned into study groups: control (no etching) and four experimental groups (20, 40, 80 and 160 s of etching). The etched surfaces’ microstructure including crystal structure, pore pattern, pore depth, and pore width was studied under a scanning electron microscope, and the surface roughness and wettability were analyzed using a non-contact surface profilometer and a contact angle measuring device, respectively. The results were statistically analyzed using one-way analysis of variance (ANOVA) and the post hoc Tukey’s test. The results showed a significant change in the pore number, pore pattern, crystal structure, surface roughness, and wettability with increased etching duration. Etching for a short time resulted in small pores, and etching for longer times resulted in wider, irregular grooves. A significant increase in the surface roughness and wettability was observed with an increase in the etching duration. The findings also suggested a strong association between the surface roughness and wettability.
This study sought to evaluate the effects of different staining solutions on the colour stability of nanocomposites compared with micro hybrid resin and to evaluate the degree of conversion of these two materials. Two different shades of two different composites were cured in polytetraflouroethylene disk rings. Coffee, tea and cola drinks were used as staining solutions, and distilled water was used as a control. Data were statistically analysed using a paired T-test with a significance level of 5%. Nano composite showed the highest degree of conversion (DC) values based on calculation of the bonded and free carbonyl peak intensities in the spectrum. The colour analysis showed that nanohybrid had the highest ΔE values when exposed to coffee solutions; they showed less color stability despite having a higher degree of conversion. Nano resin composite showed significantly higher discoloration than microhybrid composite.
Osteochondroma of the mandibular condyle is fairly rare. We describe a case of this lesion in a 52-year-old woman who presented with symptoms of temporomandibular joint dysfunction. Although a panoramic radiograph demonstrated the bony exostosis, a pre-operative CT examination showed the relationship of the tumour to the condyle and also depicted soft-tissue changes secondary to the growth.
The current study was aimed to fabricate customized root form dental implant using additive manufacturing technique for the replacement of missing teeth. The root form dental implant was designed using Geomagic™ and Magics™, the designed implant was directly manufactured by layering technique using ARCAM A2™ electron beam melting system by employing medical grade Ti-6Al-4V alloy powder. Furthermore, the fabricated implant was characterized in terms of certain clinically important parameters such as surface microstructure, surface topography, chemical purity and internal porosity. Results confirmed that, fabrication of customized dental implants using additive rapid manufacturing technology offers an attractive method to produce extremely pure form of customized titanium dental implants, the rough and porous surface texture obtained is expected to provide better initial implant stabilization and superior osseointegration.
Background: Tumor markers, designated as a broad group of substances produced by malignancies, could be in the form of biochemical substances, immunological substances, cell surface changes and genetic alterations. Cancer, a disorder of cellular behavior is characterized by alteration of serum glycoproteins. L-fucose, a hexose, which is the terminal sugar in most of the plasma glycoproteins, may be useful as a tumor marker for the detection, monitoring and prognostic assessment of malignancies. The aim of the study was to ascertain the role of serum fucose as a biomarker for early detection of oral cancer and to compare serum fucose levels in healthy controls, leukoplakia and oral cancer patients. Materials and Methods: The study included 60 (100.0%) subjects, who were grouped as 20 (33.3%) control subjects, 20 (33.3%) squamous cell carcinoma patients and 20 (33.3%) leukoplakia patients. Fucose estimation was done using UV-visible spectrophotometry based on the method as adopted by Winzler using cysteine reagent. The results were analyzed statistically using ANOVA with Bonferroni post hoc tests. Results: Results showed a high significance in serum fucose in oral squamous cell carcinoma (OSCC) and leukoplakia subjects compared to normal controls. There was a gradual increase in the values noted from control to leukoplakia and to squamous cell carcinoma. Conclusions: Estimation of serum fucose may be a reliable marker and can be used as an effective diagnostic biomarker in oral squamous cell carcinoma patients.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.