The most progress towards a practical method of fusing municipal waste incineration ash has been in the use of a plasma jet that employs arc discharge, a form of thermal plasma. However, a remaining problem is that stable plasma generation is prevented by melting of the nozzle of the plasma-jet torch by the high-temperature plasma flow. With the objective of developing high-speed fusion treatment for waste materials using an in-liquid plasma jet, basic research was conducted on plasma stability and the durability of plasma-jet torches, including electrodes and nozzles. Basic plasma jet characteristics such as the discharge voltage, current, and power value at the time of plasma jet generation were investigated experimentally. The relationship between the temperature distribution near the tip of a plasma jet torch and electrode damage was investigated by fluid-heat coupled analysis using the finite element method.
Currently, novel method to synthesize diamond film on material substrate called as in-liquid microwave plasma CVD (IL-MPCVD) has been achieved. It has been studied and improved in addition expected as new method instead of conventional gas phase microwave plasma CVD (MPCVD). The purpose of this study is to synthesize single crystal diamond using IL-MPCVD in high speed deposition. The experimental conditions, methanol was poured in to the reactor. Each of diamond particles (100) and (111) was embedded on the stainless steel substrates (SUS632J2). It was mounted to the substrate holder of in-liquid plasma equipment and installed on the top cover. The distance between the tip of the electrode and the substrate was kept to 1.5mm. A microwave of 2.45GHz was irradiated into the quartz glass tube reactor from the rectangular cavity resonator with 4 mm diameter tungsten electrode and the plasma was generated at its tip. The microwave was adjusted in appropriate power to maintain a certain substrate temperature. Diamond films were evaluated by Raman spectroscopy, Scanning Electron Microscope (SEM) and Laser Microscope (LM). As a result, the best orientation for epitaxial growth was found to be (100) which have film growth gradually and smooth surface. Whereas (111) face has polycrystalline film with irregularity growth and rough surface. The remaining H and C after CO synthesis satisfying H/C>20 is necessary to synthesized diamond using IL-MPCVD. The deposition rate was about 32 μm/h when both single crystal and polycrystalline diamond film were synthesized.
Diamond-like-carbon (DLC) films are promising as coating materials. Ion plating, an excellent method in terms of adhesiveness, step coverage, and deposition rate, can form not only pure metal films but also oxide films, nitride films, and carbonized films. In this study, which aimed to form a DLC film with good adhesiveness and a diamond crystal structure, a DLC film, with a SiC interlayer formed by ion plating with introduction of tetramethylsilane (TMS), was formed. It was experimentally revealed that as the interlayer thickness increases, the crystal structure in the DLC film becomes more diamond rich, and the adhesiveness of the DLC film and substrate is thereby improved.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.