Results of studies on the modification of AlSi7Mg alloy with an exotherimc modifier are presented in the paper. MgO, Cr 2 O 3 , Na 2 O 2 , NaNO 3 , Na 2 MoO 4 were used as modifiers in the amount of 0.05, 0.10, 0.15, 0.20 and 0.25%, and Cr 2 O 3 +Al, NaNO 3 +Al, Na 2 MoO 4 +Al were applied as exothermic modifiers with Al as the reducing agent in the amount of 0.04-0.3%. The analyzed modifiers were incorporated in line with factorial design 2 3 . The Inmold modification method was applied. The microstructure of selected modified alloys was presented, and their tensile strength, percentage elongation and Brinell hardness number were given in graphic form. The results of the study indicate that the use of modifiers delivering an exothermic effect influences the effectiveness of silumin modification.Keywords: Al alloys, modification, silumin, exothermic modifier W pracy przedstawiono wyniki badań nad modyfikacją stopu AlSi7Mg modyfikatorem egzotermicznym. Do badań użyto, jako modyfikatorów związków MgO, Cr 2 O 3 , Na 2 O 2 , NaNO 3 , Na 2 MoO 4 wprowadzanych w ilości 0.05, 0.10, 0.15, 0.20 and 0.25% oraz w postaci modyfikatora egzotermicznego z Al jako reduktorem Cr 2 O 3 +Al, NaNO 3 +Al i Na 2 MoO 4 +Al w ilości 0.04-0.3% wprowadzanych zgodnie z planem czynnikowym 2 3 . Modyfikację prowadzono metodą Inmold. Przedstawiono wybrane mikrostruktury stopu po modyfikacji oraz w postaci graficznej wytrzymałość na rozciąganie, wydłużenie procentowe i twardość Brinella. Wykazano, że zastosowanie modyfikatora w postaci mieszanki dającej efekt egzotermiczny wpływa na efektywność modyfikacji siluminu.