The functionalization of Multi-walled Carbon Nanotubes (MWCNTs) is addressed to improve its interaction capability with other materials for further applications. The oxidation of MWCNTs by nitric acid is one of the promising methods for its surface modifications. In this research, MWCNTs functionalization was carried out in several steps such as oxidation, filtration, washing, and drying. The optimization of reaction time for MWCNTs functionalization was conducted to achieve the optimum condition which efficiently functionalizes MWCNTs surface. The sample characterizations were investigated by Boehm titration, Fourier Transform Infrared (FTIR) Spectroscopy, Thermo Gravimetric Analysis (TGA), and dispersion test. As a result, carboxyl groups were successfully attached onto the MWCNTs surface and stable dispersion of MWCNTs was obtained after 12 hours. Oxidation with nitric acid for 12 hours at room temperature is the optimum treatment time for surface modification.
Ketersediaan lignin yang melimpah dan efisiensi biaya, lignosulfonat dapat digunakan sebagai stabilisasi surfaktan. Penelitian ini melakukan sintesis surfaktan lignosulfonat dan lignosulfonat teraminasi dengan tujuan untuk menghasilkan gugus sulfonat pada lignin alkali standar dan gugus amina pada lignosulfonat standar serta mengetahui nilai tegangan antarmuka lignosulfonat teraminasi hasil sintesis. Metode yang digunakan adalah sulfonasi lignin alkali standar menggunakan reaksi substitusi elektrofilik dan aminasi lignosulfonat standar menggunakan reaksi Mannich. Lignosulfonat hasil sintesis akan dikarakterisasi menggunakan FTIR (Fourier Transform Infrared) dan lignosulfonat teraminasi hasil sintesis akan dikarakterisasi menggunakan FTIR dan IFT (Interfacial Tension) tensiometer. Karakterisasi lignosulfonat hasil sintesis menggunakan FTIR menunjukkan adanya perbedaan kemunculan vibrasi ikatan dengan lignin alkali standar. Perbedaan dapat terlihat dengan adanya vibrasi ikatan S=O sulfat pada bilangan gelombang 1420,78 cm-1 dan C-S-O pada bilangan gelombang 623,37 cm-1 pada lignosulfonat hasil sintesis. Karakterisasi FTIR lignosulfonat teraminasi hasil sintesis menunjukkan adanya vibrasi ikatan N-H pada bilangan gelombang 3258,62 cm-1 dan vibrasi ikatan C-N pada bilangan gelombang 1214,45 cm-1. Kedua vibrasi ikatan tersebut tidak dapat ditemukan pada hasil analisis FTIR lignosulfonat standar. Hasil pengukuran IFT menunjukkan nilai tegangan antarmuka lignosulfonat teraminasi hasil sintesis sebesar 2,124 mN/M. Nilai tegangan antarmuka lignosulfonat teraminasi hasil sintesis yang lebih rendah dari lignin alkali hasil isolasi tandan kosong kelapa sawit dan lignosulfonat standar menunjukkan bahwa penggunaan amina primer berupa etilendiamin dapat mempengaruhi lipofilisitas lignosulfonat teraminasi sebagai surfaktan.
Bio ethanol is one of the potential fuels in the future. However, ethanol in water mixture has an azeotropic concentration of 95.6 wt. %, which makes it difficult to purify further. The common method of purification is by using an azeotropic distillation column, which requires an intensive energy and an addition of specific solvent. In this study, ethanol purification is done using an adsorption column packed with zeolite Raschig rings. The natural zeolite ring was modified beforehand using the NaOH solution to enhance the material's water adsorption performance. The ethanol purity can reach more than 99% with the modified zeolite packing. The modification also increases the saturation time of the packed bed column, thus making it more efficient. AbstractPemurnian Etanol dengan Zeolit Alam Teraktivasi. Bio ethanol adalah salah satu bahan bakar potensial di masa depan. Namun campuran etanol dalam air memiliki titik azeotrop pada konsentrasi 95,6 % berat, sehingga sulit untuk dimurnikan lebih lanjut. Metode umum yang dipakai dalam pemurnian etanol adalah menggunakan kolom distilasi azeotropik yang membutuhkan energi yang intensif dan penambahan solven tertentu. Pada penelitian ini, pemurnian etanol dilakukan dengan kolom adsorpsi dengan bahan isian cincin zeolite di dalamnya. Zeolit alam sebelum digunakan dimodifikasi dengan larutan NaOH agar kemampuan penjerapan (adsorpsi) air menjadi meningkat. Kemurnian etanol dapat mencapai lebih dari 99% dengan zeolite termodifikasi. Modifikasi ini juga meningkatkan waktu saturasi kolom sehingga kolom bisa dijalankan dengan efisien.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.