The Ono's rotary bending fatigue test and the cantilever rotary bending fatigue test were carried out on friction-welded 6061 aluminum alloy joints, and the relationship between the deformation heat input in the upset stage or the upset burn-off length and fatigue strength was examined. In the Ono's type test, sound joints, which fractured in the heat affected zone in the tensile test, fractured in the heat affected zone also and the fatigue limit of these joints was slightly lower than that of 6061 aluminum alloy base metal. This is because joints fractured in the softened area in both tensile test and Ono's type test using smoothed test specimens. While, in the cantilever type test, the fatigue limit of sound joints was a little more than or a little less than that of 6061 aluminum alloy base metal. It seems that a weld and a structure at the weld interface affected fatigue strength in the cantilever type test using notched test specimens. Judging from the fatigue limit obtained, sound joints could be produced when either the deformation heat input in the upset stage or the upset burn-off length exceeded a certain value.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.