XRD and FTIR crystallinity indices in sound human tooth enamel and synthetic hydroxyapatite

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

8
102
0
2

Year Published

2016
2016
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 171 publications
(112 citation statements)
references
References 26 publications
8
102
0
2
Order By: Relevance
“…In amorphous calcium phosphate, due to lattice distortion, PO 4 vibration bending mode is usually seen as a single broad band [39]. The finding of the present study indicated better crystallinity and bigger crystal size of NeoMTA Plus than of MTA Angelus [38]. The crystallinity index of both NeoMTA Plus and MTA Angelus (4.8 ± 0.37 and 3.7 ± 0.52, resp.)…”
Section: Discussionmentioning
confidence: 44%
See 3 more Smart Citations
“…In amorphous calcium phosphate, due to lattice distortion, PO 4 vibration bending mode is usually seen as a single broad band [39]. The finding of the present study indicated better crystallinity and bigger crystal size of NeoMTA Plus than of MTA Angelus [38]. The crystallinity index of both NeoMTA Plus and MTA Angelus (4.8 ± 0.37 and 3.7 ± 0.52, resp.)…”
Section: Discussionmentioning
confidence: 44%
“…The crystallinity index of both NeoMTA Plus and MTA Angelus (4.8 ± 0.37 and 3.7 ± 0.52, resp.) falls in the range recorded for synthetic hydroxyapatite (3.6-6.07), but it is generally higher than that recorded for sound human tooth enamel (3.23) [38].…”
Section: Discussionmentioning
confidence: 52%
See 2 more Smart Citations
“…This was also confirmed by recording the ATR spectra of physical mixtures of HA and chitosan containing from 1% to 30% of chitosan; in all cases the characteristic peaks of chitosan were not visible (data not shown). The crystallinity index calculated from the infrared data, using a method previously described [21,22] (Table 3), showed that the control HA and the HA prepared in the presence of CNTs had similar crystallinity to fresh bone and enamel, as reported by Reyes-Gasga et al [23]; however, the presence of only polymer induced a decrease in the crystallinity index. XRD patterns of the composites (Figs.…”
Section: Synthesis and Characterisation Of Ha Compositessupporting
confidence: 64%