Abstract: Inorganic materials have been extensively studied for visible electrochromism in the past few decades. However, the single inorganic electrochromic (EC) material commonly exhibits a single color change, leading to a narrow spectrum of modulation, which offsets or limits the maximally energy-saving ability. Here, we present a wide-spectrum modulated EC device designed by combining the complementary EC nanocomposite of manganese dioxide (MnO 2 ) and Prussian blue (PB) for enhanced energy savings. Porous MnO 2 na… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

1
46
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 72 publications
(52 citation statements)
references
References 59 publications
(90 reference statements)
1
46
0
Order By: Relevance
“…The cluster morphology was different from that in the Prussian blue film and MnO 2 /PB composite films as stated in previous studies. 42,43 It is explained that the MnO 2 nanoparticle was also uniformly deposited on a reduced Prussian white (PW) cluster, not only on a film surface. From the lower-resolution SEM image of PW@MnO 2 , the crack gap interval was dotted with a spherical cluster on the film surface (Figure S5c).…”
Section: Electrochromic Performance Of the Electrochromic Energy Stor...mentioning
confidence: 99%
See 1 more Smart Citation
“…The cluster morphology was different from that in the Prussian blue film and MnO 2 /PB composite films as stated in previous studies. 42,43 It is explained that the MnO 2 nanoparticle was also uniformly deposited on a reduced Prussian white (PW) cluster, not only on a film surface. From the lower-resolution SEM image of PW@MnO 2 , the crack gap interval was dotted with a spherical cluster on the film surface (Figure S5c).…”
Section: Electrochromic Performance Of the Electrochromic Energy Stor...mentioning
confidence: 99%
“…In contrast to the tedious preparation method in the literature, PW@MnO 2 can be obtained facilely by step-by-step electrodeposition within 8 min in this work, while there was at least 9 h for one-time formation of the MnO 2 film in the literature. 42 The common electrochromic cathodic material WO 3 acted as the EESD negative electrode and was prepared by magnetron sputtering. A flexible Li-based solid-state EESD was successfully fabricated by the electrolyte solidification method.…”
Section: Introductionmentioning
confidence: 99%
“…Electrochromic smart windows can present different color response when different voltage was inputted, and it is attracting increasing interest for reducing the building energy consumption [58][59][60][61][62] . In comparison with rigid ECDs, flexible ECDs can be installed onto the pristine glass window without replacing all windows 63 .…”
Section: Introductionmentioning
confidence: 99%
“…Electrochromic devices (ECDs) have attracted increased attention in smart windows, displays and color-tuneable optical elements because of their zero energy consumption when at various working states ( Ma et al, 2021 ; Kim et al, 2021 ; Cui et al, 2019 ; Seong et al, 2018 ; Park et al, 2017 ; Wu et al, 2021 ). Especially, multicolor electrochromic displays are one of the most versatile applications because they can retain their colored states without the need to supply electrical power.…”
Section: Introductionmentioning
confidence: 99%