Vacuum heat treatment of electroless Ni–B coatings

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

5
79
0
4

Year Published

2010
2010
2023
2023

Publication Types

Select...
8
2

Relationship

0
10

Authors

Journals

citations
Cited by 122 publications
(88 citation statements)
references
References 4 publications
5
79
0
4
Order By: Relevance
“…Among these elements nickel based coatings play a major role in our everyday lives for decorative and industrial applications. Low temperature heat treatment of nickel coatings resulted higher wear resistance which equal or exceeds that of hard chromium coatings [4]. Properties such as corrosion resistance, better strength at high and low temperature, high hardness [5] and high wear resistance make nickel a suitable candidate for mechanical parts subject to abrasion and erosion.…”
Section: Methodsmentioning
confidence: 99%
“…Among these elements nickel based coatings play a major role in our everyday lives for decorative and industrial applications. Low temperature heat treatment of nickel coatings resulted higher wear resistance which equal or exceeds that of hard chromium coatings [4]. Properties such as corrosion resistance, better strength at high and low temperature, high hardness [5] and high wear resistance make nickel a suitable candidate for mechanical parts subject to abrasion and erosion.…”
Section: Methodsmentioning
confidence: 99%
“…pH of the electroless nickel bath is demanded between 12 to 14 and the reduction reaction is expected as following [11]; (1) Furthermore, as a complexing agent ethylenediamine were used to prevent precipitation of nickel hydroxide. As a stabilizer lead tungstate were utilized to control the reactions on the substrate [12].…”
mentioning
confidence: 99%
“…Electroless Ni-B coating has an amorphous structure [20,21]. The structure of electroless Ni-B coating crystallized after the plasma nitriding treatments at the different temperatures same as heat treatment [22][23][24][25]. When XRD patterns were analyzed, it was observed that Ni 3 B phase predominated in the structure of plasma nitrided CP-Ti which was initially coated electroless Ni-B at 500…”
Section: Xrd Analysismentioning
confidence: 99%