Synthesis and optical characterization of CdTe nanocrystals prepared by ball milling process

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4

Citation Types

0
22
0

Year Published

2006
2006
2023
2023

Publication Types

Select...
4
3
2

Relationship

0
9

Authors

Journals

citations
Cited by 47 publications
(22 citation statements)
references
References 19 publications
0
22
0
Order By: Relevance
“…Many properties of nanoparticles depend on their size and shape (Li et al, 2002; Tan et al, 2003; Zhang et al, 2010). Fiber-shaped (one-dimensional) nanoparticles exhibit different properties than round-shaped (zero-dimensional) nanospheres (Hamilton et al, 2009; Tafen et al, 2009; Wu et al, 2010; Zhi et al, 2011).…”
Section: Introductionmentioning
confidence: 99%
“…Many properties of nanoparticles depend on their size and shape (Li et al, 2002; Tan et al, 2003; Zhang et al, 2010). Fiber-shaped (one-dimensional) nanoparticles exhibit different properties than round-shaped (zero-dimensional) nanospheres (Hamilton et al, 2009; Tafen et al, 2009; Wu et al, 2010; Zhi et al, 2011).…”
Section: Introductionmentioning
confidence: 99%
“…Structural evolution or phase transition have also been observed in these mono-dispersive CdSe nanocrystals upon critical static pressures [35,36], the wurtzite CdSe nanocrystals performed similar phase transition to rock salt structure like bulk crystal. Recently, mechanical alloying (MA) process has been applied to synthesize CdTe nanocrystals [37][38][39] and many other types of nanocrystals [40,41]. Non-hydrostatic pressure induced phase transformation has also been observed in the alloyed compounds during ball milling process [42].…”
Section: Introductionmentioning
confidence: 99%
“…MA method provides a good pathway to produce surface clean semiconductor nanocrystals, which could be used to study the intrinsic valence electronic structure and optical excitation behavior of quantum dots. Surface clean samples may be able to exclude the influence of capping organic ligand on the physical properties of the semiconductor nanocrystals [37,39]. This is a safe, low cost and easy way to fabricate semiconductor nanocrystals, and can be easily extended to mass production.…”
Section: Introductionmentioning
confidence: 99%
“…This last form of CdTe can also be obtained by the pressure cycle method [9]. In a recent paper, CdTe nanocrystals have been successfully synthesized by mechanical alloying (MA) process [10], starting from high purity elemental powders (99.99% cadmium and 99.999% tellurium). A high energy SPEX 8000D Mix/miller and a high ball-to-powder mass ratio (20:1) were used for milling times as longer as 50 h, when the particle size ranged from 2 to 6 nm.…”