Synthesis and characterization of pH-sensitivity semi-IPN hydrogel based on hydrogen bond between poly(N-vinylpyrrolidone) and poly(acrylic acid)

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

3
72
0

Year Published

2008
2008
2019
2019

Publication Types

Select...
7
2

Relationship

1
8

Authors

Journals

citations
Cited by 141 publications
(77 citation statements)
references
References 23 publications
3
72
0
Order By: Relevance
“…The main peaks of AA are -OH stretch at 3380 cm -1 , -CH stretch at 2922 cm -1 and -C=O stretch at 1718.5 cm -1 (Ranjha et al, 2011). PVP shows peaks at 2924 cm -1 for CH stretching, a stretching peak between 1650 to 1659 cm -1 for carbonyl stretching (C=O) and 1290 cm -1 for amide band III (C-N stretch) (Jin et al, 2006). In the FTIR spectrum ( Figure 2), carbonyl bands in complex were broader than in pure PVP and AA, and are evidence of intermolecular hydrogen bonding.…”
Section: Fourier Transform Infrared (Ftir) Spectroscopymentioning
confidence: 97%
“…The main peaks of AA are -OH stretch at 3380 cm -1 , -CH stretch at 2922 cm -1 and -C=O stretch at 1718.5 cm -1 (Ranjha et al, 2011). PVP shows peaks at 2924 cm -1 for CH stretching, a stretching peak between 1650 to 1659 cm -1 for carbonyl stretching (C=O) and 1290 cm -1 for amide band III (C-N stretch) (Jin et al, 2006). In the FTIR spectrum ( Figure 2), carbonyl bands in complex were broader than in pure PVP and AA, and are evidence of intermolecular hydrogen bonding.…”
Section: Fourier Transform Infrared (Ftir) Spectroscopymentioning
confidence: 97%
“…Owing to their super strong water absorption ability, they have been extensively used in agriculture and forestry, construction, medical [4,5] and public health, and daily life supplies [6][7][8][9]. In fact,~90% of superabsorbent hydrogels are disposable products [10,11], and most of them are synthesized by the graft copolymerization between hydrophilic monomers with double bond such as acrylic acid (AA) and acrylamide (AM).…”
Section: Introductionmentioning
confidence: 99%
“…The semi-IPN hydrogels showed a lower swelling capacity of 13 g/g at pH 2, and then abruptly jump to 120 g/g around pH 4. This behavior was typical property of pH-sensitive hydrogel [19]. The COO -groups were protonated to form COOH groups when pH was lower than 4 due to the pKa of 4.25 of -COOH [20], thus the hydrogen between the carboxylic groups and the amide groups kept polymer chains of the hydrogels close to each other and restricted the expansion of the network.…”
Section: Swelling Of Semi-ipn Hydrogels -Effect Of Phmentioning