2022
DOI: 10.1016/j.actamat.2021.117607
|View full text |Cite
|
Sign up to set email alerts
|

Stress corrosion cracking resistant nanostructured Al-Mg alloy with low angle grain boundaries

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
22
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 85 publications
(22 citation statements)
references
References 58 publications
0
22
0
Order By: Relevance
“…The original structure absorbed tensile forces to transform into the tensile structure, resulting in dislocation from the low AGB to the high AGB in the X-direction [55]. If the tensile stress was located under the elastic zone or before the strain at break, the tensile structure would return to the original structure by releasing forces, resulting in dislocation from the high AGB to the low AGB in the X-direction [56]. These reversible transformed structures and forces also occurred in the Y-direction.…”
Section: Forces and Displacements Analysis For Internal Structure Cha...mentioning
confidence: 99%
“…The original structure absorbed tensile forces to transform into the tensile structure, resulting in dislocation from the low AGB to the high AGB in the X-direction [55]. If the tensile stress was located under the elastic zone or before the strain at break, the tensile structure would return to the original structure by releasing forces, resulting in dislocation from the high AGB to the low AGB in the X-direction [56]. These reversible transformed structures and forces also occurred in the Y-direction.…”
Section: Forces and Displacements Analysis For Internal Structure Cha...mentioning
confidence: 99%
“…Numerous studies show that the corrosion properties of aluminum alloys are dominated by grain boundary precipitates, which depends on the grain boundary structure [ 32 , 33 ]. According to the literature [ 34 ], the corrosion resistance of aluminum alloys can be enhanced by increasing the low-angle grain boundaries to inhibit the alloy’s precipitation of GBPs. Moreover, the width of the PFZ also has a significant impact on the corrosion performance of alloys.…”
Section: Discussionmentioning
confidence: 99%
“…Besides residual compressive stress, the size and Figure 6 HAADF image of IGC of the unaffected AA7150 substrate and the corresponding EDS mapping after immersion in 3.5 Wt.% NaCl solution at room temperature for 6 h distribution of grain boundary precipitates also closely related to SCC resistance. Xu et al (2022) obtained an average grain size of 500 nm in Al-5Mg by using dynamic plastic deformation, which generated a quantity of low angle grain boundaries (LAGBs), and the LAGBs can significantly restrain the precipitation of Mg-rich particles along grain boundaries. As a result, the SCC resistance of Al-5Mg was promoted by a wide margin.…”
Section: Effect Of Surface Severe Plastic Deformation On Stress Corro...mentioning
confidence: 99%