Starch/chitosan films reinforced with polydopamine modified MMT: Effects of dopamine concentration

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
20
0
1

Year Published

2017
2017
2022
2022

Publication Types

Select...
5
2
1

Relationship

0
8

Authors

Journals

citations
Cited by 65 publications
(23 citation statements)
references
References 25 publications
0
20
0
1
Order By: Relevance
“…TGA was used to estimate the intercalation extent of the Mt by ε-PL, as well as the thermal stability of the Mt, ε-PL and PL-Mt [37]. As illustrated in Figure 3, the Mt exhibited excellent thermal stability, with a residue as high as 90.78% at 800 • C, and a pronounced mass loss from ambient to 100 • C owing to the evaporation of absorbed water.…”
Section: Tga Of Pl-mtmentioning
confidence: 99%
“…TGA was used to estimate the intercalation extent of the Mt by ε-PL, as well as the thermal stability of the Mt, ε-PL and PL-Mt [37]. As illustrated in Figure 3, the Mt exhibited excellent thermal stability, with a residue as high as 90.78% at 800 • C, and a pronounced mass loss from ambient to 100 • C owing to the evaporation of absorbed water.…”
Section: Tga Of Pl-mtmentioning
confidence: 99%
“…In this research, PDA as a synthetic analogue of the naturally occurring melanin was prepared through dopamine autopolymerization and it is biocompatible and environmentally friendly . The incorporation of PDA remarkably improved compatibility and adhesion between nano SiO 2 and PP matrix which is mainly responsible for excellent mechanical properties . The incorporation of modified SiO 2 nano‐particle SiO 2 @polydopamine also tremendously improved hydrophilicity of PP matrix that may contribute to dyeing of PP product .…”
Section: Introductionmentioning
confidence: 99%
“…which is mainly responsible for excellent mechanical properties. 21 The incorporation of modified SiO 2 nano-particle SiO 2 @ polydopamine also tremendously improved hydrophilicity of PP matrix that may contribute to dyeing of PP product. [22][23][24][25] When 1% wt SiO 2 @polydopamine and a certain amount of b nucleating agent was added, the impact strength of composite reached the maximum value 12.60 k J/m 2 (improving 127% compared to pure PP), the bending strength reached 41.85 MPa, the bending modulus was 2192 MPa, the composite possessed hydrophilic performance with the water contact angle of 88.328.…”
Section: Introductionmentioning
confidence: 99%
“…With an increase in the SL concentration, the weight loss of the TiO 2 ‐SLx samples increased, especially for TiO 2 ‐SL25. Therefore, the addition of SL decreased the thermal stability of TiO 2 ‐SLx (Zhou et al., ).…”
Section: Resultsmentioning
confidence: 99%