“…In a typical procedure, the AEMWE system consists of an anode (NiFe LDHs/Ni fiber, 2 × 2 cm 2 ), a cathode (0.4 mg cm −2 of 70 wt.% Pt/C) coated on the anion exchange membrane (A201, Tokuyama, 2 × 2 cm 2 ), and a gas diffusion layer (carbon paper, Toray) [17][18][19]. Then, the anode, the cathode, an alkaline anion exchange membrane, and carbon paper were hot-pressed at 60 • C and 0.1 MPa for 2 min to obtain membrane electrode assembly (NiFe LDHs/Ni fiber || Pt/C) [20,21].…”