Role of silica mid-layer in thermal and chemical stability of hierarchical Fe3O4-SiO2-TiO2 nanoparticles for improvement of lead adsorption: Kinetics, thermodynamic and deep XPS investigation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

3
20
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 68 publications
(23 citation statements)
references
References 45 publications
3
20
0
Order By: Relevance
“…These findings demonstrate the presence of Fe 3+ and Fe 2+ , which appeared as a result of mixing biochar with iron oxide. Satellite peaks of Fe 3+ and Fe 2+ were found at the range of binding energy of 715-720 eV, which is similar to the results of Naeemeh et al[80] and Haixia Wu et al[81]. Figure10cshows that after adsorption of Cd(II), there was a significant displacement of Fe 2p binding energy, implying the occurrence of coordination reactions between Fe and Cd.Figure10shows the broad peaks of magnetic biochar (after adsorption), C1s spectrum, O1s spectrum, Fe2p spectrum, and Cdp2 spectrum.…”
supporting
confidence: 87%
“…These findings demonstrate the presence of Fe 3+ and Fe 2+ , which appeared as a result of mixing biochar with iron oxide. Satellite peaks of Fe 3+ and Fe 2+ were found at the range of binding energy of 715-720 eV, which is similar to the results of Naeemeh et al[80] and Haixia Wu et al[81]. Figure10cshows that after adsorption of Cd(II), there was a significant displacement of Fe 2p binding energy, implying the occurrence of coordination reactions between Fe and Cd.Figure10shows the broad peaks of magnetic biochar (after adsorption), C1s spectrum, O1s spectrum, Fe2p spectrum, and Cdp2 spectrum.…”
supporting
confidence: 87%
“…The peaks located at 711.4 eV and 724.1 eV which belong to Fe 3+ 2p 3/2 and 2p 1/2 [72] . Deconvolution of the peak areas shows that the ratio of Fe 3+ /Fe 2+ was 1.92, comparable to the molar ratio of Fe 3+ /Fe 2+ in Fe 3 O 4 [73] . To conclude, the characterizations of XRD, 57 Fe Mössbauer and XPS confirm that co‐process of bio‐oil with RM could efficiently transform Fe 2 O 3 and FeOOH to Fe 3 O 4 .…”
Section: Resultsmentioning
confidence: 79%
“…In addition, CTAB can also improve the stability of the magnetic material in aqueous solution and facilitate the TiO 2 layer arranging on Fe–Al MMH [ 33 ]. TiO 2 provides high surface area and protects Fe–Al MMH surface from oxidation [ 34 , 35 ]. The surface area of the sorbents was measured and calculated by Brunauer-Emmett-Teller method.…”
Section: Resultsmentioning