Reduction effect of final-pass heavy reduction rolling on the texture development, tensile property and stretch formability of ZWK100 alloy plates

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2022
2022
2023
2023

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 12 publications
(3 citation statements)
references
References 59 publications
0
3
0
Order By: Relevance
“…values were observed for the three sheets prepared according to different rolling parameters. Some studies have shown that the formability of a sheet is strongly dependent on its microstructure, texture, and plastic deformation mechanism during stretch forming [ 17 , 27 ]. Therefore, in this study, it was necessary to systematically investigate the three sheets’ microstructures and texture evolution as well as their plastic deformation mechanisms during stretch forming.…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…values were observed for the three sheets prepared according to different rolling parameters. Some studies have shown that the formability of a sheet is strongly dependent on its microstructure, texture, and plastic deformation mechanism during stretch forming [ 17 , 27 ]. Therefore, in this study, it was necessary to systematically investigate the three sheets’ microstructures and texture evolution as well as their plastic deformation mechanisms during stretch forming.…”
Section: Resultsmentioning
confidence: 99%
“…In addition, Shi et al investigated the effect of different final-pass rolling reduction methods on the microstructure and properties of Mg–1.1Zn–0.76Y–0.56Zr alloy, finding that increasing the final-pass rolling reduction can modify the TD-split texture, achieving the reduction of planar anisotropy. When they increased the final-pass rolling reduction from 30% to 70%, the Erichsen value increased from 7.0 mm to 8.0 mm [ 16 , 17 ]. The reasons for the weakening of texture by thermomechanical processing are complex.…”
Section: Introductionmentioning
confidence: 99%
“…What's more, annealing process is also an effective way to modify the microstructure and texture [27,28]. The ZWK100 alloy can form a weak texture and achieve low planar anisotropy by final-pass heavy reduction rolling and subsequent annealing [29]. The double-peak texture tilted to RD of multi-pass hotrolled AZMX1100 alloy can transform into an elliptical annular texture at low annealing temperatures while a uniform weak elliptical annular texture at high annealing temperature of 400 °C [30].…”
Section: Introductionmentioning
confidence: 99%