“…The peaks at 1,384 and 1,464 cm −1 corresponded to the bending vibration of C-H, whereas the peaks at 2,853 and 2,924 cm −1 corresponded to the stretching vibration of C-H (Liu et al , 2022a, 2022b). The peak at 1,026 cm −1 corresponded to the stretching vibration of Si-O-Si (Wang et al , 2022a, 2022b, 2022c), and the peaks at 1,636 and 3,412 cm −1 corresponded to the bending and stretching vibrations of O-H (Wu et al , 2023), respectively. This also indicated the successful deposition of polysiloxane on the surface.…”