Preparation and thermal properties of metal matrix composites with wood-structure

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2010
2010
2024
2024

Publication Types

Select...
5

Relationship

1
4

Authors

Journals

citations
Cited by 7 publications
(1 citation statement)
references
References 19 publications
0
1
0
Order By: Relevance
“…Obviously, the SiC peak appeared along with the carbon peak. This is because the silicone resin in the netlike carbon was firstly decomposed into silicone compound (Si x O y ) between 400 and 650 • C, and the SiC was formed at the temperature exceeding 1400 • C through the reaction of the carbon with silicone compound [13,14]. This indicates that it is a mixed material, i.e.…”
Section: Microstructuresmentioning
confidence: 99%
“…Obviously, the SiC peak appeared along with the carbon peak. This is because the silicone resin in the netlike carbon was firstly decomposed into silicone compound (Si x O y ) between 400 and 650 • C, and the SiC was formed at the temperature exceeding 1400 • C through the reaction of the carbon with silicone compound [13,14]. This indicates that it is a mixed material, i.e.…”