Polymeric films containing pomegranate peel extract based on PVA/starch/PAA blends for use as wound dressing: In vitro analysis and physicochemical evaluation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
23
0
1

Year Published

2020
2020
2023
2023

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 54 publications
(24 citation statements)
references
References 59 publications
0
23
0
1
Order By: Relevance
“…In the case of PD, different thermal events were observed with peak temperatures ranging between 100 and 235 °C, which were associated to the loss of surface water and volatile low molar mass components of the dye (approximately 12 wt% of the initial mass) [49]. Other losses were also observed at temperatures around 235 °C and 440 °C, which were probably related to the loss of organic material and thermal decomposition of the different components present in PD [50] which were degraded to phenolic acids and aldehydes by deglycosylation and ring opening reactions [51]. This behaviour indicates a poor high temperature resistance for the studied natural pigment.…”
Section: Thermal Stability Of Pdnpsmentioning
confidence: 99%
“…In the case of PD, different thermal events were observed with peak temperatures ranging between 100 and 235 °C, which were associated to the loss of surface water and volatile low molar mass components of the dye (approximately 12 wt% of the initial mass) [49]. Other losses were also observed at temperatures around 235 °C and 440 °C, which were probably related to the loss of organic material and thermal decomposition of the different components present in PD [50] which were degraded to phenolic acids and aldehydes by deglycosylation and ring opening reactions [51]. This behaviour indicates a poor high temperature resistance for the studied natural pigment.…”
Section: Thermal Stability Of Pdnpsmentioning
confidence: 99%
“…Therefore, it cannot be surprising that different materials of unique properties and forms are applied in modern dressings. Especially polymers, of both synthetic and natural origin, garner great attention in the field; among the naturally occurring polymers employed in dressing production, chitosan [107], hyaluronic acid [108], keratin [109], gelatin, starch [110], silk fibroin [111], heparin [112,113], collagen [114], sericin [115], sodium alginate [116,117], zein [118], and konjac glucomannan [119][120][121] can be enumerated [122,123]. On the other hand, polyvinyl alcohol (PVA) [110], polylactic acid (PLA) [124], polyacrylic acid (PAA) [110], polyethylene glycol (PEG) [125], polycaprolactone (PCL) [126], and polyvinylpyrrolidone (PVP) [127] are examples of synthetic polymers applied for that purpose [128].…”
Section: Modern Wound Dressing Materials and Nanomaterialsmentioning
confidence: 99%
“…The swelling index, Q, was investigated in phosphate-buffered solution (PBS) over 60 min, at room temperature, according to the procedure adopted from Costa et al [35]. PVA/TPS packaging samples, with dimensions of 50 mm × 15 mm × 0.01 mm, were dried in an oven at 105 • C until a constant mass was reached, after which the samples were placed in vials containing 50 mL of PBS solution.…”
Section: Study Of Filmsmentioning