Oxidation behaviors of low carbon MgO‐C refractories: Roles of Ti2AlC and Ti2AlN

Abstract: In this study, Ti 2 AlC/Ti 2 AlN powders were first incorporated to fabricate lowcarbon MgO-C refractories, and their oxidation behaviors were investigated. Computed tomography (CT) results indicated that stress cracks only occurred in the Ti 2 AlC-added sample after exposure to 1100 • C, and the anomalous oxidation behavior of Ti 2 AlC powder at 578 • C worsened the oxidation result at 1100 • C for MgO-C refractories with Ti 2 AlC. At 1500 • C, the oxidation behaviors of MgO-Ti 2 AlC/Ti 2 AlN-C samples reveal… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 6 publications
(1 citation statement)
references
References 55 publications
(104 reference statements)
0
1
0
Order By: Relevance
“…19 For the R1 films subjected to heat treatment at various temperatures, Ti 2 AlN crystal structures were detected at 13° (002), 34.6° (100), and 40° (103). 2023 Additionally, TiN phases were observed at 36.8° (111) and 42.7° (200), accompanied by a TiO 2 phase at 41.8° (111). Following annealing at 800°C, the presence of TiO 2 became more pronounced.…”
Section: Resultsmentioning
confidence: 99%
“…19 For the R1 films subjected to heat treatment at various temperatures, Ti 2 AlN crystal structures were detected at 13° (002), 34.6° (100), and 40° (103). 2023 Additionally, TiN phases were observed at 36.8° (111) and 42.7° (200), accompanied by a TiO 2 phase at 41.8° (111). Following annealing at 800°C, the presence of TiO 2 became more pronounced.…”
Section: Resultsmentioning
confidence: 99%