“…1a. 33 Figure 1b shows the diffraction peak of GO was not appeared and the alternative broad diffraction peak was observed in the region of 24°to 28°indicating the graphene oxide was reduced and form as the reduced graphene oxide. 34 002),( 111), (020), ( 200), ( 022), ( 112), ( 113), ( 221), ( 222), ( 131), ( 223), ( 312), ( 402), ( 241), ( 110), ( 135), ( 044), ( 511), ( 510), ( 350) and (424) matched with the standard JCPDS Card No: 73-1032.…”