2009
DOI: 10.1016/j.tws.2008.12.008
|View full text |Cite
|
Sign up to set email alerts
|

Numerical study of axially crushed cylindrical tubes with corrugated surface

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

1
10
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 49 publications
(11 citation statements)
references
References 10 publications
1
10
0
Order By: Relevance
“…However, tube with a¼ 0.5 mm showed an initial peak force as a result of having more straight axial geometry. When corrugation amplitude was increased from 0.5 mm to 2 and 3 mm, mean force decreased significantly ( $34% for a¼ 2 mm and $ 51% for a ¼3 mm) as also reported by Chen and Ozaki [25]. This can be attributed to increase in the curvature of the corrugation and transition of diamond collapse mode to concertina progressive collapse mode through corrugations with increasing corrugation amplitude as depicted in Fig.…”
Section: Crashworthiness Of Empty Straight and Corrugated Tubessupporting
confidence: 78%
See 2 more Smart Citations
“…However, tube with a¼ 0.5 mm showed an initial peak force as a result of having more straight axial geometry. When corrugation amplitude was increased from 0.5 mm to 2 and 3 mm, mean force decreased significantly ( $34% for a¼ 2 mm and $ 51% for a ¼3 mm) as also reported by Chen and Ozaki [25]. This can be attributed to increase in the curvature of the corrugation and transition of diamond collapse mode to concertina progressive collapse mode through corrugations with increasing corrugation amplitude as depicted in Fig.…”
Section: Crashworthiness Of Empty Straight and Corrugated Tubessupporting
confidence: 78%
“…In last decades, to improve the crashworthiness of thin-walled tubes, several modification methods have been developed and proposed. Among those, filling tubes with different cellular materials or structures including metallic foams [4][5][6][7][8][9][10], synthetic foams [11][12][13][14][15], natural cellular materials [16] and honeycombs [17], multi-tube usage [17][18][19][20][21][22] and generating corrugated/grooved surfaces on the tubes [13,[23][24][25][26][27][28][29][30] were found to be very effective to increase energy absorption capacity and structure safety.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Moreover, geometric modification from a straight tube (S-tube) to a single-sided radial corrugated tube (SSC) has shown a desirable smooth load-displacement behavior with minimal fluctuations [40][41][42][43][44][45][46][47]. The introduction of corrugations helped in directing the crushing energy to the corrugation trough.…”
Section: Introductionmentioning
confidence: 99%
“…Acar et al [13] investigated the effects of tapering and introducing axisymmetric indentations on the crash performances of thinwalled tubes. Numerical simulations conducted by Chen et al [14] showed that the deformation modes corresponding to corrugations can be classified into axisymmetric and asymmetric modes. In addition, Chen et al [15] studied the circumferential strain concentrations in cylindrical and square tubes with corrugated surfaces under axial compression.…”
Section: Introductionmentioning
confidence: 99%