2004
DOI: 10.1016/j.surfcoat.2003.05.004
|View full text |Cite
|
Sign up to set email alerts
|

Nano-crystalline filtered arc deposited (FAD) TiAlN PVD coatings for high-speed machining applications

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
27
0

Year Published

2009
2009
2022
2022

Publication Types

Select...
5
2

Relationship

0
7

Authors

Journals

citations
Cited by 55 publications
(34 citation statements)
references
References 15 publications
0
27
0
Order By: Relevance
“…This process is dissipative structures. Such real broken dependences are described, for example, for cutting tool [25,26]. In [25,26] and in Figure 1c,d friction conditions allow passage of self-organization, i.e., the thermodynamic stability of the tribosystem may be lost under these conditions.…”
Section: The Physical Meaning Of the Self-organization Phenomenon As mentioning
confidence: 99%
See 3 more Smart Citations
“…This process is dissipative structures. Such real broken dependences are described, for example, for cutting tool [25,26]. In [25,26] and in Figure 1c,d friction conditions allow passage of self-organization, i.e., the thermodynamic stability of the tribosystem may be lost under these conditions.…”
Section: The Physical Meaning Of the Self-organization Phenomenon As mentioning
confidence: 99%
“…Such real broken dependences are described, for example, for cutting tool [25,26]. In [25,26] and in Figure 1c,d friction conditions allow passage of self-organization, i.e., the thermodynamic stability of the tribosystem may be lost under these conditions. The loss of thermodynamic stability, therefore, and self-organization are stochastic processes (due to the fact that compliance with the conditions of Lyapunov's theorem) is necessary but not sufficient) [20].…”
Section: The Physical Meaning Of the Self-organization Phenomenon As mentioning
confidence: 99%
See 2 more Smart Citations
“…As outlined above, these amorphous films, which are SS-I, have high plasticity and improved lubricating properties [130]. Under more severe cutting conditions (machining of annealed 1045 steel at cutting speeds of 250-450 m min −1 ) cemented carbide tooling has been used with TiAlN nanocrystalline coatings [186]. A more complex phenomenon takes place on the friction surface.…”
Section: Tribofilms (Secondary Structures)mentioning
confidence: 99%