Microstructure and mechanical properties of bulk Mg–Zn–Ca amorphous alloys and amorphous matrix composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
20
0

Year Published

2009
2009
2016
2016

Publication Types

Select...
6
2
1

Relationship

0
9

Authors

Journals

citations
Cited by 49 publications
(21 citation statements)
references
References 26 publications
1
20
0
Order By: Relevance
“…1a shows unclear contrast in the backscatter electron scanning image, which indicated the pure amorphous structure of alloy I. [14,15,17]. However, with a spot of Fe particle addition, alloy II displayed an almost entirely dendritic morphology (Fig.…”
Section: Resultsmentioning
confidence: 97%
See 1 more Smart Citation
“…1a shows unclear contrast in the backscatter electron scanning image, which indicated the pure amorphous structure of alloy I. [14,15,17]. However, with a spot of Fe particle addition, alloy II displayed an almost entirely dendritic morphology (Fig.…”
Section: Resultsmentioning
confidence: 97%
“…The Mg-Zn-Ca metallic glass system has been extensively investigated [14,15]. However, Mg-Zn-Ca glassy alloys are extremely brittle at room temperature as well as require the use of high-purity metallic elements and strict environmental conditions because the scantling of oxygen or other impurities dramatically deteriorate the glass forming ability (GFA).…”
Section: Introductionmentioning
confidence: 99%
“…Conversely, MgZnCa bulk metallic glass composites (BMGCs) were found to present much lower corrosion rates than the other Mg-based crystalline alloys. Unfortunately, monolithic MgZnCa bulk metallic glasses are quite brittle, limiting their further applications [2][3][4][5][6]. There have hitherto been a number of studies reporting on effective methods that enhance the strength as well as the plasticity of Mg-based BMGCs through the dispersion of ductile metallic particles such as those of Mo, Fe, Nb, and Ti [7][8][9][10][11][12][13][14][15][16][17].…”
Section: Introductionmentioning
confidence: 99%
“…The as-cast (5 mm) composite exhibits some large fragments after fracture and abides by the "fragmentation mode," which usually occurs in brittle alloys (Fig. 7c) [29]. The fracture surface of the as-annealed Cu 47.5 Zr 47.5 Al 5 BMG composite consists of many steep slipped planes and some fractured crevices (Fig.…”
Section: Cuzrmentioning