2013
DOI: 10.1016/j.jeurceramsoc.2013.01.027
|View full text |Cite
|
Sign up to set email alerts
|

Microstructural and mechanical investigation of hydroxyapatite–zirconia nanocomposites prepared by spark plasma sintering

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
6
0

Year Published

2015
2015
2021
2021

Publication Types

Select...
7
1

Relationship

1
7

Authors

Journals

citations
Cited by 14 publications
(9 citation statements)
references
References 20 publications
1
6
0
Order By: Relevance
“…The hardness of pure HAP sintered at 600°C showed 3.9 ± 0.2 GPa and 3 point bending strength was 58 ± 5 MPa from our previous work [36]. This fact proves that the addition of graphene may the positive effect of mechanical properties of composite.…”
Section: Thermodynamic Calculationsupporting
confidence: 61%
“…The hardness of pure HAP sintered at 600°C showed 3.9 ± 0.2 GPa and 3 point bending strength was 58 ± 5 MPa from our previous work [36]. This fact proves that the addition of graphene may the positive effect of mechanical properties of composite.…”
Section: Thermodynamic Calculationsupporting
confidence: 61%
“…Gergely et al [51] studied microstructural and mechanical properties of ZrO 2 /HAp nanocomposites obtained by spark plasma sintering (SPS). To prevent the reaction between ZrO 2 and nHAp and decomposition of nHA, the SPS method was carried out at short dwelling time (5 min) and low temperatures.…”
Section: Hap-zirconia Nanocompositementioning
confidence: 99%
“…The density of the pure HA increased from 2.31±0.02 to 3.06±0.02 g/cm 3 . The density of the pure HA sintered at 1300 °C is reasonably close to the theoretical density of 3.156 g/cm 3 for the HA ceramics [74].…”
Section: Resultsmentioning
confidence: 94%