2010
DOI: 10.1134/s0040579510040251
|View full text |Cite
|
Sign up to set email alerts
|

Mechanical activation of α-spodumene for further processing into lithium compounds

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
10
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 29 publications
(11 citation statements)
references
References 0 publications
0
10
0
Order By: Relevance
“…After heating the amorphous spodumene metastable c-form appears approximately at 800°C which is subsequently converted into b-spodumene at higher temperatures between 900 and 1080°C depending on the experimental conditions (Nordmann and Cheng, 1997;Guo et al, 2006;Kotsupalo et al, 2010;Gasalla et al, 1987). Ferro et al (2004) observed that a rare Li zeolite bikitaite [Li 2 (Al 2 Si 4 O 12 )Á2H 2 O, P1] transforms to c-spodumene at temperature of 800°C and Hurlbut (1957) found the transformation of bikitaite to b-spodumene upon heating to 900°C.…”
Section: Phase Transformation Via C-spodumenementioning
confidence: 98%
See 1 more Smart Citation
“…After heating the amorphous spodumene metastable c-form appears approximately at 800°C which is subsequently converted into b-spodumene at higher temperatures between 900 and 1080°C depending on the experimental conditions (Nordmann and Cheng, 1997;Guo et al, 2006;Kotsupalo et al, 2010;Gasalla et al, 1987). Ferro et al (2004) observed that a rare Li zeolite bikitaite [Li 2 (Al 2 Si 4 O 12 )Á2H 2 O, P1] transforms to c-spodumene at temperature of 800°C and Hurlbut (1957) found the transformation of bikitaite to b-spodumene upon heating to 900°C.…”
Section: Phase Transformation Via C-spodumenementioning
confidence: 98%
“…Amorphization is performed via melting with alloying elements (Nordmann and Cheng, 1997) or via mechanical treatment (Kotsupalo et al, 2010;Gasalla et al, 1987). After heating the amorphous spodumene metastable c-form appears approximately at 800°C which is subsequently converted into b-spodumene at higher temperatures between 900 and 1080°C depending on the experimental conditions (Nordmann and Cheng, 1997;Guo et al, 2006;Kotsupalo et al, 2010;Gasalla et al, 1987).…”
Section: Phase Transformation Via C-spodumenementioning
confidence: 99%
“…It is stated that grinding cleaves the Li-O, Al-O, and Si-O-Si bonds from the tetrahedral site. It shows that the α-spodumene turns into γ-spodumene between 700 and 900 • C before transitioning into β-spodumene between 900 and 950 • C [81]. This would mean a decrease in the energy necessary to decrepitate the spodumene but does not consider the amount of energy needed to grind the material.…”
Section: Conversion Processes Of Spodumenementioning
confidence: 99%
“…[9][10][11] This polymorph is also formed when the mechanically activated a phase is annealed at temperatures between 700 1C and 900 1C. [11][12][13] Like b-spodumene, g-spodumene is absent in nature but it can be produced relatively easily from melts. 14 It has hexagonal symmetry with Si and Al occupying the centre of tetrahedrons; its density is 2400 kg m À3 .…”
Section: Introductionmentioning
confidence: 99%