2005 IEEE Antennas and Propagation Society International Symposium
DOI: 10.1109/aps.2005.1552844
|View full text |Cite
|
Sign up to set email alerts
|

Measurement of the dielectric properties of Rogers R/flex 3850 liquid crystalline polymer substrate in V and W band

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
5
0

Publication Types

Select...
5
3

Relationship

0
8

Authors

Journals

citations
Cited by 12 publications
(5 citation statements)
references
References 2 publications
0
5
0
Order By: Relevance
“…It was observed that TC-PPO- g -PB2 exhibits low D k and D f in the tested frequency range (10–110 GHz). Its D k value of TC-PPO- g -PB2 are superior to that of previously reported commercial LCP materials, which exhibited a D k of 3.16 over the similar frequency range, while D f of TC-PPO- g -PB2 is higher than 0.0049 observed in commercial LCP materials . Notably, upon examination of the dielectric properties of TC-PPO- g -PB2 around 10 GHz using SCR and BCDR methods, slight variations in D k and D f were observed.…”
Section: Resultsmentioning
confidence: 51%
See 1 more Smart Citation
“…It was observed that TC-PPO- g -PB2 exhibits low D k and D f in the tested frequency range (10–110 GHz). Its D k value of TC-PPO- g -PB2 are superior to that of previously reported commercial LCP materials, which exhibited a D k of 3.16 over the similar frequency range, while D f of TC-PPO- g -PB2 is higher than 0.0049 observed in commercial LCP materials . Notably, upon examination of the dielectric properties of TC-PPO- g -PB2 around 10 GHz using SCR and BCDR methods, slight variations in D k and D f were observed.…”
Section: Resultsmentioning
confidence: 51%
“…Its D k value of TC-PPO-g-PB2 are superior to that of previously reported commercial LCP materials, which exhibited a D k of 3.16 over the similar frequency range, while D f of TC-PPO-g-PB2 is higher than 0.0049 observed in commercial LCP materials. 52 Notably, upon examination of the dielectric properties of TC-PPO-g-PB2 around 10 GHz using SCR and BCDR methods, slight variations in D k and D f were observed. This disparity can be inferred from the fact that SCR evaluates the in-plane component of the sample dielectric property, whereas BCDR measures the dielectric property perpendicular to the sample.…”
Section: Dielectric Properties Of Ppo-g-pb Filmsmentioning
confidence: 99%
“…23(a). After comparing the S 21 between measurement and simulation results, the extracted loss tangent is 0.053, as compared to 0.0067 at 98.5 GHz [40]. Fig.…”
Section: Measurement Results and Discussionmentioning
confidence: 99%
“…The PCB is gold plated afterwards to be able to apply wire-bonding. In [32], [33] the electrical properties of LCP substrate is measured and estimated, with a dielectric constant of 3.2 and a loss tangent of around 0.005 at 80 GHz. We have used these values in the modeling and all simulations.…”
Section: Antenna Designmentioning
confidence: 99%