Liquid Phase Morphology Control of ZnO Nanowires, Ellipse Particles, Hexagonal Rods, and Particle in Aqueous Solutions

Abstract: Liquid phase morphology control of ZnO crystals was realized with simple aqueous solution system. ZnO nanowires were successfully fabricated at 50• C. They were over 50 μm in length and about 100 nm in width. Aspect ratio was estimated to be over 500. They had no branches and were obtained without aggregations. Curved nano-wires clearly indicated high flexibility and high mechanical strength. Additionally, ellipse particles, hexagonal rods and particles were fabricated in the solutions. Morphology, crystal gro… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2

Citation Types

0
2
0

Year Published

2013
2013
2022
2022

Publication Types

Select...
2
1

Relationship

1
2

Authors

Journals

citations
Cited by 3 publications
(2 citation statements)
references
References 44 publications
(49 reference statements)
0
2
0
Order By: Relevance
“…Recently, aqueous solution process was established as next‐generation science and technology. Various structures of SnO 2 , TiO 2 , ZnO, etc. were synthesized in the solutions.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Recently, aqueous solution process was established as next‐generation science and technology. Various structures of SnO 2 , TiO 2 , ZnO, etc. were synthesized in the solutions.…”
Section: Introductionmentioning
confidence: 99%
“…Recently, aqueous solution process was established as next-generation science and technology. Various structures of SnO 2 , [15][16][17][18][19][20] TiO 2 , [21][22][23][24][25][26][27][28][29][30][31][32][33][34][35][36][37][38] ZnO, [39][40][41][42][43][44][45][46][47][48] etc. were synthesized in the solutions.…”
Section: Introductionmentioning
confidence: 99%