Iron-Cobalt Coatings Produced Using an Eco-friendly Route

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

1
2
0
3

Year Published

2022
2022
2023
2023

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(6 citation statements)
references
References 34 publications
1
2
0
3
Order By: Relevance
“…Previously, we showed that varying the composition of the bath for chemical deposition (the Fe : Co ratio, the type of reducing agent) enables to synthesize FeCo−C coatings with a thickness of up to 4 µm with a uniform distribution of elements, with the ability to control surface morphology and grain size (15−300 nm) [14]. In this article, the chemical deposition method enabled to synthesize both metal films of FeCo(C) alloys (Fig.…”
Section: Resultsmentioning
confidence: 87%
See 1 more Smart Citation
“…Previously, we showed that varying the composition of the bath for chemical deposition (the Fe : Co ratio, the type of reducing agent) enables to synthesize FeCo−C coatings with a thickness of up to 4 µm with a uniform distribution of elements, with the ability to control surface morphology and grain size (15−300 nm) [14]. In this article, the chemical deposition method enabled to synthesize both metal films of FeCo(C) alloys (Fig.…”
Section: Resultsmentioning
confidence: 87%
“…However, the use of traditional reducing agents (hypophosphite or sodium borohydride) leads to significant contamination of the deposited coatings with phosphorus and boron, which leads to deterioration of magnetic characteristics. The use of natural polysaccharides (chitosan, cellulose, arabinogalactan) as reducing agents can become a simple, environmentally friendly and technological method for creating unique nanostructured functional materials [10][11][12][13][14].…”
Section: Introductionmentioning
confidence: 99%
“…Ранее мы показали, что варьирование состава ванны для химического осаждения (соотношение Fe : Со, тип восстановителя) позволяет синтезировать покрытия FeСо−C толщиной до 4 µm с однородным распределением элементов, с возможностью управлять морфологией поверхности и размером зерна (15−300 nm) [14]. В данной работе, метод химического осаждения позволил синтезировать как металлические пленки сплавов FeСо(C) (рис.…”
Section: результаты и обсуждениеunclassified
“…3), а значения величин K V и k S покрытий FeCo−C, полученные в результате такого описания, представлены в таблице. Видно, что вклад объемной анизотропии возрастает с увеличением содержания кобальта в сплаве FeCo, что коррелирует с увеличением размера зерен (определяемого из данных РФА и электронной микроскопии) [14].…”
Section: результаты и обсуждениеunclassified
See 1 more Smart Citation