Homochiral MOF–Polymer Mixed Matrix Membranes for Efficient Separation of Chiral Molecules

Abstract: Homochiral metal–organic framework (MOF) membranes have been recently reported for chiral separations. However, only a few high‐quality homochiral polycrystalline MOF membranes have been fabricated due to the difficulty in crystallization of a chiral MOF layer without defects on porous substrates. Alternatively, mixed matrix membranes (MMMs), which combine potential advantages of MOFs and polymers, have been widely demonstrated for gas separation and water purification. Here we report novel homochiral MOF–poly… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
11
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 35 publications
(11 citation statements)
references
References 52 publications
0
11
0
Order By: Relevance
“…In derivative thermogravimetric (DTG) curves (Figure S7), a significant peak is observed in the temperature range of 253−390 °C for NH 2 -MOFs/TiNM, corresponding to the pyrolysis of His molecules. 24 However, no obvious peak in this range is observed in MOFs/TiNM. From 253 to 390 °C, the weight loss values of NH 2 -MOFs/ TiNM and MOFs/TiNM are 5.69 and 5.37% (Figure 3C).…”
Section: ■ Results and Discussionmentioning
confidence: 98%
See 3 more Smart Citations
“…In derivative thermogravimetric (DTG) curves (Figure S7), a significant peak is observed in the temperature range of 253−390 °C for NH 2 -MOFs/TiNM, corresponding to the pyrolysis of His molecules. 24 However, no obvious peak in this range is observed in MOFs/TiNM. From 253 to 390 °C, the weight loss values of NH 2 -MOFs/ TiNM and MOFs/TiNM are 5.69 and 5.37% (Figure 3C).…”
Section: ■ Results and Discussionmentioning
confidence: 98%
“…Thermogravimetric analysis further verifies the incorporated ligands in NH 2 -MOFs/TiNM. In derivative thermogravimetric (DTG) curves (Figure S7), a significant peak is observed in the temperature range of 253–390 °C for NH 2 -MOFs/TiNM, corresponding to the pyrolysis of His molecules . However, no obvious peak in this range is observed in MOFs/TiNM.…”
Section: Results and Discussionmentioning
confidence: 99%
See 2 more Smart Citations
“…These membranes have advantages of providing high surface area, varying functionalities, tunable and pore size. Due to multitude of properties, these are widely used in drug delivery systems, chemical sensors, gas storage and catalysis ( Lu et al, 2019 ).…”
Section: Applicationsmentioning
confidence: 99%