High-Performance Supercapacitor Electrode Based on Buckypaper/Polyaniline Composite

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

0
9
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 14 publications
(9 citation statements)
references
References 20 publications
0
9
0
Order By: Relevance
“…FTIR spectra are shown in Figure . The FTIR spectra for all samples present typical peaks of cellulose at 896 cm –1 (C–H bending), 1031 cm –1 (C–O stretching), 1162 cm –1 (C–O stretching), 1429 cm –1 (alkane C–H bending), 1640 cm –1 (O–H bending of absorbed water), 2897 cm –1 (C–H stretching), and 3333 cm –1 (O–H stretching). ,, PANI gives typical peaks at 798 cm –1 (aromatic C–H out-of-plane bending), 1123 cm –1 (aromatic C–H in-plane bending), 1298 cm –1 (aromatic amine C–N stretching), 1485 cm –1 (benzenoid ring CC stretching), 1566 cm –1 (quinoid ring CC stretching), and 3437 cm –1 (N–H stretching), indicating that PANI is in the emeraldine salt state. ,, These peaks can be observed on the spectra for PANI, nanocellulose/PANI, and nanocellulose/PANI/RGO, indicating that PANI has been successfully coated on the nanocellulose substrate. RGO shows peaks at 690 cm –1 (C–H bending), 1402 cm –1 (C–H bending), and 3138 cm –1 (O–H stretching). ,, Also PANI is adsorbed onto RGO through the amino groups of aniline by alkane bending (1429 cm –1 ), C–H stretching (2897 cm –1 ), and O–H stretching (3333 cm –1 ), indicating that both PANI and RGO have been successfully loaded on the nanocellulose substrate …”
Section: Resultsmentioning
confidence: 93%
“…FTIR spectra are shown in Figure . The FTIR spectra for all samples present typical peaks of cellulose at 896 cm –1 (C–H bending), 1031 cm –1 (C–O stretching), 1162 cm –1 (C–O stretching), 1429 cm –1 (alkane C–H bending), 1640 cm –1 (O–H bending of absorbed water), 2897 cm –1 (C–H stretching), and 3333 cm –1 (O–H stretching). ,, PANI gives typical peaks at 798 cm –1 (aromatic C–H out-of-plane bending), 1123 cm –1 (aromatic C–H in-plane bending), 1298 cm –1 (aromatic amine C–N stretching), 1485 cm –1 (benzenoid ring CC stretching), 1566 cm –1 (quinoid ring CC stretching), and 3437 cm –1 (N–H stretching), indicating that PANI is in the emeraldine salt state. ,, These peaks can be observed on the spectra for PANI, nanocellulose/PANI, and nanocellulose/PANI/RGO, indicating that PANI has been successfully coated on the nanocellulose substrate. RGO shows peaks at 690 cm –1 (C–H bending), 1402 cm –1 (C–H bending), and 3138 cm –1 (O–H stretching). ,, Also PANI is adsorbed onto RGO through the amino groups of aniline by alkane bending (1429 cm –1 ), C–H stretching (2897 cm –1 ), and O–H stretching (3333 cm –1 ), indicating that both PANI and RGO have been successfully loaded on the nanocellulose substrate …”
Section: Resultsmentioning
confidence: 93%
“…57,59,60 RGO shows peaks at 690 cm −1 (C−H bending), 1402 cm −1 (C−H bending), and 3138 cm −1 (O−H stretching). 57,59,60 Impact of TA Concentrations on Performance of SCs. To investigate the impact of TA concentrations on electrochemical performance of SCs, the self-healable GelMA-CNC hydrogels were treated with 40%, 60%, 80%, and 100% TA, respectively, for 24 h. The results are shown in Figure 5a and c−e.…”
Section: ■ Results and Discussionmentioning
confidence: 98%
“…The peaks in the spectrum of GelMA include amide I, II, and III groups at 1612, 1520, and 1436 cm –1 , respectively . GelMA-CNC presents typical peaks at 896 cm –1 (C–H bending), 1031 cm –1 (C–O stretching), 1162 cm –1 (C–O stretching), 1429 cm –1 (alkane C–H bending), 1640 cm –1 (O–H bending of absorbed water), and 2897 cm –1 (C–H stretching). ,, TA-GelMA-CNC showed a typically wave at around 3000–3600 cm –1 which is closely related to the formation of hydrogen bonds due to the wavenumber of amine N–H and the galloyl O–H shift in this range. The peak value 3309 cm –1 (GelMA) shifted to 3269 cm –1 (GelMA-TA), indicating the formation of H-bonding .…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…The capacitance of the MWCNTs/polyaniline electrode was observed to be 329 F g -1 at 10 mVs -1 . For comparison, Tran et al reported a potentially better-performing supercapacitor based on the in-situ electropolymerization of polyaniline at buckypaper (397 Fg -1 at 10 mV s -1 )66 . Furthermore, Gross et al observed clear performance differences with FAD-GDH based bioanodes with different mediators6 .…”