Graphite-based lithium ion battery with ultrafast charging and discharging and excellent low temperature performance

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
92
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 118 publications
(92 citation statements)
references
References 31 publications
0
92
0
Order By: Relevance
“…Then the white sediment was obtained and washed by anhydrous ethanol 3 times, then heated at 80 °C for 8 hours in vacuum. In order to obtain high crystallinity LTO NSs, the white precursor was calcined in a horizontal tube furnace at 600 °C for 6 hours with air atmosphere …”
Section: Methodsmentioning
confidence: 99%
See 4 more Smart Citations
“…Then the white sediment was obtained and washed by anhydrous ethanol 3 times, then heated at 80 °C for 8 hours in vacuum. In order to obtain high crystallinity LTO NSs, the white precursor was calcined in a horizontal tube furnace at 600 °C for 6 hours with air atmosphere …”
Section: Methodsmentioning
confidence: 99%
“…In order to obtain high crystallinity LTO NSs, the white precursor was calcined in a horizontal tube furnace at 600°C for 6 hours with air atmosphere. [4] LTO/Ag composition: The silver nanocrystals were distributed on LTO NSs via a facile electroless deposition procedure. [42] First, a Tollens' reagent was prepared by dropping diluted NH 4 OH into an AgNO 3 solution (0.005 M) until the original sediment dissolved.…”
Section: Methodsmentioning
confidence: 99%
See 3 more Smart Citations