2010
DOI: 10.1007/978-90-481-9419-3_11
|View full text |Cite
|
Sign up to set email alerts
|

Grammatical Evolution and STE Criterion

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
15
0

Year Published

2016
2016
2019
2019

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 10 publications
(15 citation statements)
references
References 2 publications
0
15
0
Order By: Relevance
“…The surface morphology consists of a number of craters [Luo 2009], [Han 2007 and also lumps of debris that were detected at 20% of the surface of the samples. The surface microcracks formed as a result of expansion processes caused by highspeed cooling were detected at 5% of the surface of the samples.…”
Section: Conclusion and Discussionmentioning
confidence: 99%
See 4 more Smart Citations
“…The surface morphology consists of a number of craters [Luo 2009], [Han 2007 and also lumps of debris that were detected at 20% of the surface of the samples. The surface microcracks formed as a result of expansion processes caused by highspeed cooling were detected at 5% of the surface of the samples.…”
Section: Conclusion and Discussionmentioning
confidence: 99%
“…The discharge causes melting of microscopic particles of material which are subsequently flushed from the discharge place by dielectric. In this way, craters are formed on the surface of the machined material and wire electrode [Ho 2004], [Abbas 2007]. The WEDM technology is used mainly for machining of parts that are complex in shape and indented and also with parts that are difficult to machine by conventional methods.…”