Flexural properties of repaired heat‐polymerising acrylic resin after wetting with monomer and acetone

Abstract: In clinical use, wetting the repair surfaces may result in stronger repairs. The use of bonding agent in VLC resin repairs in combination with wetting agent results in improved flexural properties.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

1
12
0
5

Year Published

2013
2013
2021
2021

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 22 publications
(19 citation statements)
references
References 22 publications
(64 reference statements)
1
12
0
5
Order By: Relevance
“…6,8,11,12 Bu düşüşün nedeninin akrilik kaide rezini ile tamir rezini arasındaki zayıf bağlantıdan olabileceği vurgulanmıştır. 8 …”
Section: Discussionunclassified
See 2 more Smart Citations
“…6,8,11,12 Bu düşüşün nedeninin akrilik kaide rezini ile tamir rezini arasındaki zayıf bağlantıdan olabileceği vurgulanmıştır. 8 …”
Section: Discussionunclassified
“…2 Akril tamirindeki başarı tamir kenarlarının yüzey şekline, tamir şekline ve tamirden önce tamir yüzeyine uygulanan işlemlere bağlıdır. 8,10,11 Hiçbir tamir işlemi orijinal akrilin dayanımına yakın dayanıma sahip olmasa da kırık yüzey üzerine uygulanabilecek çeşitli mekanik ve kimyasal ön işlemlerin yüzey morfolojisini veya kimyasını değiştirerek daha iyi bağlantı sağlayabildikleri çeşitli araştırmalarda gösterilmiştir. 8,[11][12][13][14][15][16] Böylelikle tamir materyali ile kırık yüzeyi arasında oluşturulabilecek güçlü bağlantı tamirin ömrünü uzatabilmektedir.…”
Section: Introductionunclassified
See 1 more Smart Citation
“…9 Adhesion between the fractured surface and the repair material can be promoted by treating the repair surfaces such as roughening or wetting with some chemicals. 10 The present study investigated the effect of joint surface treatment on the flexural strength of repaired autopolymerized acrylic resin. Many studies have investigated the repair of thermo-polymerized acrylic denture.…”
Section: Discussionmentioning
confidence: 99%
“…Delamination results not only in the loss of tissue adaptation, but also decreases the mechani-cal strength of the relined denture 4,5,[8][9][10] . Chemical surface treatment of the denture base resin can enhance the diffusion and penetration of the monomer, and thus improve bonding 6,7,[11][12][13][14][15][16][17][18][19][20][21][22][23][24][25][26][27][28][29][30] . Chloroform 6,13,14 and methylene chloride 6,12,[14][15][16][17][18][19] have been suggested as chemical surface treatment agents, but there is evidence that they may be carcinogenic to humans 31 .…”
Section: Introductionmentioning
confidence: 99%