“…Ag 3 PO 4 can be fabricated by different methods, such as precipitation [54][55][56][57], ion exchange [58], hydrotherm [59], electrochemical oxidation [60], and etc. Bi et al [54] prepared Ag 3 PO 4 with size less than 1μm by liquid phase deposition.…”